| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 2.40e+13 ohm-cm | 2.40e+13 ohm-cm | 60°C for 500 hrs |
|
Fujipoly Industries Sarcon® 30H Thin-Film HR
Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of ..
|
|||
| Volume Resistivity | 2.40e+13 ohm-cm | 2.40e+13 ohm-cm | 60°C for 500 hrs |
|
Fujipoly Industries Sarcon® 45H Thin-Film HR
Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of ..
|
|||
| Volume Resistivity | 2.40e+13 ohm-cm | 2.40e+13 ohm-cm | ASTM D247 |
|
Plenco 2369 Phenolic, Granular, Compression Molded
PLENCO 02369 is a general purpose, organic filled phenolic molding compound, formulated to minimize the generation of free ammonia for applications that are sensitive to such formation. PLENCO 02369..
|
|||
| Volume Resistivity | 2.40e+13 ohm-cm | 2.40e+13 ohm-cm | ASTM D247 |
|
Plenco 3557 Phenolic, Granular, Compression Molded
PLENCO 03557 is a woodflour and mineral filled phenolic molding compound offering excellent dielectric strength values at elevated temperatures while maintaining mechanical strength properties. UL r..
|
|||
| Volume Resistivity | 2.40e+13 ohm-cm | 2.40e+13 ohm-cm | |
|
Resinlab® EP1296 Highly Filled, Moderately Thixotropic Black Casting Resin
Resinlab™ EP1296 is a highly filled, moderately thixotropic black casting resin designed for applications requiring good thermal conductivity, low shrinkage and a low CTE. It was especially formula..
|
|||