Polymer Property : Volume Resistivity = 4.00e+16 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most.
Electrical Properties Metric English Comments
Volume Resistivity 4.00e+16 ohm-cm
4.00e+16 ohm-cm
ASTM D257
Ravago Manufacturing Americas Hylex® P1307L Polycarbonate
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..
Volume Resistivity 4.00e+16 ohm-cm
4.00e+16 ohm-cm
ASTM D257
Ravago Manufacturing Americas Hylex® P1310G30 HB Polycarbonate, 30% Fiberglass Reinforced, UV Stabilized
Information provided by Ravago.
Volume Resistivity 4.00e+16 ohm-cm
4.00e+16 ohm-cm
500V; Ø 93x3mm; IEC 60093
SYNTHOS Forsan® 573 Acrylonitrile Butadiene Styrene (ABS)
Increased heat resistant, glossy, good mechanical properties, suitable for electroplating.Applications: Electrotechnics, automotiveHousehold appliances, electric switches, car interior parts, profil..
Volume Resistivity >= 4.00e+16 ohm-cm
>= 4.00e+16 ohm-cm
ASTM D257
SABIC Innovative Plastics Valox® 310 PBT (Asia Pacific)
Unreinforced, general purpose. Typical viscosity 5000-7000.
Volume Resistivity >= 4.00e+16 ohm-cm
>= 4.00e+16 ohm-cm
ASTM D257
SABIC Innovative Plastics Valox® 311 PBT
Unreinforced, improved resistance to UV. Medium viscosity.
Volume Resistivity >= 4.00e+16 ohm-cm
>= 4.00e+16 ohm-cm
ASTM D257
SABIC Innovative Plastics Valox® 325 PBT
General purpose, unreinforced, improved processing. Applications like sprinklers and nozzles, pumps, door handle, tank covers, pens, pencils etc.
Volume Resistivity 4.00e+16 ohm-cm
4.00e+16 ohm-cm
IEC 60093
SABIC Innovative Plastics Valox® VX7024 PBT (Europe-Africa-Middle East)
VALOX VX7024 is a 12% mineral filled PBT injection moulding resin with excellent mechanical properties.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Volume Resistivity 4.00e+16 ohm-cm
4.00e+16 ohm-cm
ASTM D257
Techmer ES HiFill® PP GF15 CC 15% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc.
Volume Resistivity 4.00e+16 ohm-cm
4.00e+16 ohm-cm
ASTM D257
Techmer ES HiFill® PP GF20 CC HS 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and Chemically CoupledInformation pro..
Volume Resistivity 4.00e+16 ohm-cm
4.00e+16 ohm-cm
ASTM D257
Techmer ES Luriblend® PP GF20 CC GL2 BK 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: Graphite Powder Lubricant(2%)Features: Chemically Coupled and LubricatedAppearance: BlackInf..
Volume Resistivity 4.00e+16 ohm-cm
4.00e+16 ohm-cm
ASTM D257
Techmer ES Luriblend® PP GF20 GL2 BK 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: Graphite Powder Lubricant(2%)Features: LubricatedAppearance: BlackInformation provided by TP..
Volume Resistivity 4.00e+16 ohm-cm
4.00e+16 ohm-cm
ASTM D257
Samyang Trirex® 3000H Polycarbonate, Low-temperature Impact
PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3000H is a low temperature impact grade.Applications: Mobile Phone Housing, high gloss..
Volume Resistivity 4.00e+16 ohm-cm
4.00e+16 ohm-cm
ASTM D257
Samyang Trirex® 3020A Polycarbonate with Heat Stabilizer
PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3020A is a high flow grade with heat stabilizers.Information provided by Samyang.
Volume Resistivity 4.00e+16 ohm-cm
4.00e+16 ohm-cm
ASTM D257
Samyang Trirex® 3020IR Polycarbonate with Heat Stabilizer
PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3020IR is a high flow grade with added heat stabilizers, separating materials and stain..
Volume Resistivity 4.00e+16 ohm-cm
4.00e+16 ohm-cm
ASTM D257
Samyang Trirex® 3022A Polycarbonate
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..
Volume Resistivity 4.00e+16 ohm-cm
4.00e+16 ohm-cm
ASTM D257
Samyang Trirex® 3022R Polycarbonate with Heat Stabilizer
PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3022R is a general use grade with heat stabilizers and separating materials added.Appli..
Volume Resistivity 4.00e+16 ohm-cm
4.00e+16 ohm-cm
ASTM D257
Samyang Trirex® 3025G15 Polycarbonate, 15% Glass Reinforced
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..
Volume Resistivity 4.00e+16 ohm-cm
4.00e+16 ohm-cm
ASTM D257
Samyang Trirex® 3025PJ Polycarbonate
PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3025PJ is a general use grade.Information provided by Samyang.
Volume Resistivity 4.00e+16 ohm-cm
4.00e+16 ohm-cm
ASTM D257
Samyang Trirex® 3027IR Polycarbonate
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..
Volume Resistivity 4.00e+16 ohm-cm
4.00e+16 ohm-cm
ASTM D257
Samyang Trirex® 3027PJ Polycarbonate
PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3027PJ is an extrusion grade.Information provided by Samyang.
Volume Resistivity 4.00e+16 ohm-cm
4.00e+16 ohm-cm
ASTM D257
Samyang Trirex® 3500G20 Polycarbonate, 20% Glass Reinforced
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..
Volume Resistivity 4.00e+16 ohm-cm
4.00e+16 ohm-cm
ASTM D257
Techmer ES HiFill® PP GF20 CC 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc.
Volume Resistivity 4.00e+16 - 4.50e+16 ohm-cm
4.00e+16 - 4.50e+16 ohm-cm
ASTM D257
SABIC Innovative Plastics NORYL FP6130 PPE+PS (Asia Pacific)
Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a..
Volume Resistivity 4.00e+16 - 4.50e+16 ohm-cm
4.00e+16 - 4.50e+16 ohm-cm
IEC 60093
SABIC Innovative Plastics NORYL FP6130 PPE+PS (Asia Pacific)
Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a..
Volume Resistivity 4.00e+16 ohm-cm
4.00e+16 ohm-cm
Tra-Con Tra-Cast 3113 General Purpose Epoxy Casting Compound
TRA-CAST 3113 is a low viscosity two-part formulation recommended for general purpose electrical potting and encapsulating applications where the combination of good mechanical thermal and electrica..
Volume Resistivity 4.00e+16 ohm-cm
4.00e+16 ohm-cm
ASTM D257
Ravago Manufacturing Americas Hylex® P1310G40 HB Polycarbonate, 40% Fiberglass Reinforced, UV Stabilized
Information provided by Ravago.
Volume Resistivity 4.00e+16 - 4.50e+16 ohm-cm
4.00e+16 - 4.50e+16 ohm-cm
IEC 60093
SABIC Innovative Plastics NORYL FP6130 PPE+PS
Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a..
Volume Resistivity 4.00e+16 - 4.50e+16 ohm-cm
4.00e+16 - 4.50e+16 ohm-cm
IEC 60093
SABIC Innovative Plastics NORYL FP6130 PPE+PS (Europe-Africa-Middle East)
Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a..
Volume Resistivity 4.00e+16 ohm-cm
4.00e+16 ohm-cm
ASTM D257
Samyang Trirex® 3025GRU30 Polycarbonate, 30% Glass Reinforced
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, electr..
Volume Resistivity 4.00e+16 ohm-cm

@Temperature 23.0 °C
4.00e+16 ohm-cm

@Temperature 73.4 °F
100V; ASTM D257
Victrex® APTIV® 1300-100G Polyetheretherketone (PEEK) Polymer Film
DescriptionAPTIV® 1300 film is the black version of unfilled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance ..