| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 7.00e+8 ohm-cm | 7.00e+8 ohm-cm | Approximate value obtained from graphical representation; CTM E043 |
|
Nanocyl PLASTICYL™ PA1503 Polyamide 6 with 1 wt% of Multi-Wall Carbon Nanotubes
PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLA..
|
|||