Polymer Property : Comparative Tracking Index = 350 V Product List

Electrical Properties

Tips: 30 items are displayed at most.
Electrical Properties Metric English Comments
Comparative Tracking Index 350 V
<br>@Thickness 3.20 mm
350 V
<br>@Thickness 0.126 in
Sol. B; IEC 112, UL 746A
Nilit Nilamid A3 H G10 50% Glass Reinforced PA66
Description: Nilamid A3 H G10 (50% Glass Reinforced) is a high strength material, that is used for structural applications. It is easy to mould, and shows outstanding stiffness and creep resistance,..
Comparative Tracking Index 350 V
<br>@Thickness 3.20 mm
350 V
<br>@Thickness 0.126 in
Sol. B; IEC 112, UL 746A
Nilit Nilamid A3 H G3 ZB 13% Glass Reinforced High Impact PA66
Description: Nilamid A3 H G3 ZB (13% Glass Reinforced) was developed for applications that require a combination of high stiffness and good elongation or impact resistance. It is widely used for app..
Comparative Tracking Index 350 V
<br>@Thickness 3.20 mm
350 V
<br>@Thickness 0.126 in
Sol. B; IEC 112, UL 746A
Nilit Nilamid A3 H G4 General Purpose 20% Glass Reinforced PA66
Description: Nilamid A3 H G4 is a general purpose, 20% glass fiber reinforced NYLON 66. This product combine good overall mechanical performance and impact strength with ease of processing.Key chara..
Comparative Tracking Index 350 V
<br>@Thickness 3.20 mm
350 V
<br>@Thickness 0.126 in
Sol. B; IEC 112, UL 746A
Nilit Nilamid A3 H5 G6 30% Glass Reinforced PA66
Description: Nilamid A3 H5 G6 has an outstanding mechanical performance and is 30% glass fiber reinforced. It is stabilized against chemical attack from peroxides and other oxidizing substances. It ..
Comparative Tracking Index 350 V
<br>@Thickness 3.20 mm
350 V
<br>@Thickness 0.126 in
Sol. B; IEC 112, UL 746A
Nilit Nilamid B3 H G7 35% Glass Fiber Reinforced PA6
Description: Nilamid B3 H G7 is a general purpose, 35% glass fiber reinforced NYLON 6. It has high mechanical performance, and also excellent moldability. Its impact performance is outstanding, so i..
Comparative Tracking Index 350 V
<br>@Thickness 3.20 mm
350 V
<br>@Thickness 0.126 in
Sol. B; IEC 112, UL 746A
Nilit Nilamid B3 H G8 40% Glass Fiber Reinforced PA6
Description: Nilamid B3 H G8 is a product that combines outstanding strength and stiffness with good moldability and good impact strength. It is widely used for structural applications.Key character..
Comparative Tracking Index 350 V
<br>@Thickness 3.20 mm
350 V
<br>@Thickness 0.126 in
Sol. B; IEC 112, UL 746A
Nilit Nilamon A3 H K8 40% Mineral Reinforced PA66
Description: Nilamon A3 H K8 combines good stiffness with low warpage. It is used for applications which need a degree of rigidity, particularly at higher temperatures, but which need to stay flat a..
Comparative Tracking Index 350 V
<br>@Thickness 3.20 mm
350 V
<br>@Thickness 0.126 in
Sol. B; IEC 112, UL 746A
Nilit Nilitop BT N Unfilled, Nucleated PBT
Description: Nilitop BT N is an unfilled, nucleated PBT that has excellent cycle times.Key characteristics: Good overall mechanical performanceLow moisture absorptionExcellent UV resistanceExcellent..
Comparative Tracking Index 350 V
<br>@Thickness 3.20 mm
350 V
<br>@Thickness 0.126 in
Sol. B; IEC 112, UL 746A
Nilit Nilamid A3 H G6 General Purpose 30% Glass Reinforced PA66
Description: Nilamid A3 H G6 is a general purpose 30% glass fiber reinforced NYLON 66 that gives an excellent combination of tensile strength, stiffness and impact strength. It is one of the most wi..
Comparative Tracking Index 350 V
<br>@Thickness 3.20 mm
350 V
<br>@Thickness 0.126 in
Sol. B; IEC 112, UL 746A
Nilit Nilamid A3 H G7 General Purpose 35% Glass Reinforced PA66
Description: Nilamid A3 H G7 is a general purpose 35% glass fiber reinforced NYLON 66 that gives an excellent combination of tensile strength, stiffness and impact strength. It is one of the most wi..
Comparative Tracking Index 350 V
<br>@Thickness 3.20 mm
350 V
<br>@Thickness 0.126 in
Sol. B; IEC 112, UL 746A
Nilit Nilamid A3 H G8 40% Glass Reinforced PA66
Description: Nilamid A3 H G8 is a high strength material, that is used for structural applications. It is easy to mould, and shows outstanding stiffness and creep resistance, even at elevated temper..
Comparative Tracking Index 350 V
<br>@Thickness 3.20 mm
350 V
<br>@Thickness 0.126 in
Sol. B; IEC 112, UL 746A
Nilit Nilamid A3 H6 G5 25% Glass Reinforced PA66
Description: Nilamid A3 H6 G5 is a 25% glass fiber reinforced NYLON 66 with a special stabilization system against hot oil and grease. As a result of this stabilization, the material has a brown nat..
Comparative Tracking Index 350 V
<br>@Thickness 3.20 mm
350 V
<br>@Thickness 0.126 in
Sol. B; IEC 112, UL 746A
Nilit Nilamid A3 H6 G6 30% Glass Reinforced PA66
Description: Nilamid A3 H6 G6 is a 30% glass fiber reinforced NYLON 66 with a special stabilization system against hot oil and grease. As a result of this stabilization, the material has a brown nat..
Comparative Tracking Index 350 V
<br>@Thickness 3.20 mm
350 V
<br>@Thickness 0.126 in
Sol. B; IEC 112, UL 746A
Nilit Nilamid B3 H G10 50% Glass Fiber Reinforced PA6
Description: Nilamid B3 H G10 is a product that combines outstanding strength and stiffness with good moldability and good impact strength. It is widely used for structural applications.Key characte..
Comparative Tracking Index 350 V
<br>@Thickness 3.20 mm
350 V
<br>@Thickness 0.126 in
Sol. B; IEC 112, UL 746A
Nilit Nilamid B3 H G6 30% Glass Fiber Reinforced PA6
Description: Nilamid B3 H G6 is a general purpose, 30% glass fiber reinforced NYLON 6 with a combination of good mechanical performance, impact strength and processability. It is one of the most wid..