| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Comparative Tracking Index |
500
V <br>@Thickness 3.20 mm
|
500
V <br>@Thickness 0.126 in
|
Sol. A; IEC 112, UL 746A |
|
Nilit Nilamid A G5 FR PH1 25% Glass Fiber Reinforced, Flame Retardant PA66
Description: Nilamid A G5 FR PH1 combines flame retardancy with outstanding mechanical performance. This product has a complete yellow card, with RTI and CTI listings. The formulation has been optim..
|
|||
| Comparative Tracking Index |
500
V <br>@Thickness 3.20 mm
|
500
V <br>@Thickness 0.126 in
|
Sol. B; IEC 112, UL 746A |
|
Nilit Nilamid A G5 FR PH1 25% Glass Fiber Reinforced, Flame Retardant PA66
Description: Nilamid A G5 FR PH1 combines flame retardancy with outstanding mechanical performance. This product has a complete yellow card, with RTI and CTI listings. The formulation has been optim..
|
|||
| Comparative Tracking Index |
500
V <br>@Thickness 3.20 mm
|
500
V <br>@Thickness 0.126 in
|
Sol. A; IEC 112, UL 746A |
|
Nilit Nilamid A3 H G10 50% Glass Reinforced PA66
Description: Nilamid A3 H G10 (50% Glass Reinforced) is a high strength material, that is used for structural applications. It is easy to mould, and shows outstanding stiffness and creep resistance,..
|
|||
| Comparative Tracking Index |
500
V <br>@Thickness 3.20 mm
|
500
V <br>@Thickness 0.126 in
|
Sol. B; IEC 112, UL 746A |
|
Nilit Nilamid A3 H G3 15% Glass Reinforced PA66
Description: Nilamid A3 H G3 is a general purpose, 15% glass fiber reinforced NYLON 66. This product combines good overall mechanical performance and impact strength with ease of processing.Key char..
|
|||
| Comparative Tracking Index |
500
V <br>@Thickness 3.20 mm
|
500
V <br>@Thickness 0.126 in
|
Sol. A; IEC 112, UL 746A |
|
Nilit Nilamid A3 H G3 ZB 13% Glass Reinforced High Impact PA66
Description: Nilamid A3 H G3 ZB (13% Glass Reinforced) was developed for applications that require a combination of high stiffness and good elongation or impact resistance. It is widely used for app..
|
|||
| Comparative Tracking Index |
500
V <br>@Thickness 3.20 mm
|
500
V <br>@Thickness 0.126 in
|
Sol. A; IEC 112, UL 746A |
|
Nilit Nilamid A3 H G4 General Purpose 20% Glass Reinforced PA66
Description: Nilamid A3 H G4 is a general purpose, 20% glass fiber reinforced NYLON 66. This product combine good overall mechanical performance and impact strength with ease of processing.Key chara..
|
|||
| Comparative Tracking Index |
500
V <br>@Thickness 3.20 mm
|
500
V <br>@Thickness 0.126 in
|
Sol. A; IEC 112, UL 746A |
|
Nilit Nilamid A3 H5 G6 30% Glass Reinforced PA66
Description: Nilamid A3 H5 G6 has an outstanding mechanical performance and is 30% glass fiber reinforced. It is stabilized against chemical attack from peroxides and other oxidizing substances. It ..
|
|||
| Comparative Tracking Index |
500
V <br>@Thickness 3.20 mm
|
500
V <br>@Thickness 0.126 in
|
Sol. A; IEC 112, UL 746A |
|
Nilit Nilamid B3 H G7 35% Glass Fiber Reinforced PA6
Description: Nilamid B3 H G7 is a general purpose, 35% glass fiber reinforced NYLON 6. It has high mechanical performance, and also excellent moldability. Its impact performance is outstanding, so i..
|
|||
| Comparative Tracking Index |
500
V <br>@Thickness 3.20 mm
|
500
V <br>@Thickness 0.126 in
|
Sol. A; IEC 112, UL 746A |
|
Nilit Nilamid B3 H G8 40% Glass Fiber Reinforced PA6
Description: Nilamid B3 H G8 is a product that combines outstanding strength and stiffness with good moldability and good impact strength. It is widely used for structural applications.Key character..
|
|||
| Comparative Tracking Index |
500
V <br>@Thickness 3.20 mm
|
500
V <br>@Thickness 0.126 in
|
Sol. A; IEC 112, UL 746A |
|
Nilit Nilamon A3 H K8 40% Mineral Reinforced PA66
Description: Nilamon A3 H K8 combines good stiffness with low warpage. It is used for applications which need a degree of rigidity, particularly at higher temperatures, but which need to stay flat a..
|
|||
| Comparative Tracking Index |
500
V <br>@Thickness 3.20 mm
|
500
V <br>@Thickness 0.126 in
|
Sol. A; IEC 112, UL 746A |
|
Nilit Nilamon B3 H7 GK 35 15% Glass Fiber, 25% Mineral Reinforced PA6
Description: Nilamon B3 H7 GK 35 provides a combination between low warpage and high stiffness, while retaining a good impact strength. It has a high heat aging resistance, so that it is suitable fo..
|
|||
| Comparative Tracking Index |
500
V <br>@Temperature 23.0 °C
|
500
V <br>@Temperature 73.4 °F
|
IEC 60112 |
|
DuPont Performance Polymers Crastin® SK609 BK851 PBT
(Unverified Data**)
Crastin® SK609 BK851 is a 50% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
|
|||
| Comparative Tracking Index |
500
V <br>@Thickness 3.20 mm
|
500
V <br>@Thickness 0.126 in
|
Sol. A; IEC 112, UL 746A |
|
Nilit Nilamid A3 H G6 General Purpose 30% Glass Reinforced PA66
Description: Nilamid A3 H G6 is a general purpose 30% glass fiber reinforced NYLON 66 that gives an excellent combination of tensile strength, stiffness and impact strength. It is one of the most wi..
|
|||
| Comparative Tracking Index |
500
V <br>@Thickness 3.20 mm
|
500
V <br>@Thickness 0.126 in
|
Sol. A; IEC 112, UL 746A |
|
Nilit Nilamid A3 H G7 General Purpose 35% Glass Reinforced PA66
Description: Nilamid A3 H G7 is a general purpose 35% glass fiber reinforced NYLON 66 that gives an excellent combination of tensile strength, stiffness and impact strength. It is one of the most wi..
|
|||
| Comparative Tracking Index |
500
V <br>@Thickness 3.20 mm
|
500
V <br>@Thickness 0.126 in
|
Sol. A; IEC 112, UL 746A |
|
Nilit Nilamid A3 H G8 40% Glass Reinforced PA66
Description: Nilamid A3 H G8 is a high strength material, that is used for structural applications. It is easy to mould, and shows outstanding stiffness and creep resistance, even at elevated temper..
|
|||
| Comparative Tracking Index |
500
V <br>@Thickness 3.20 mm
|
500
V <br>@Thickness 0.126 in
|
Sol. A; IEC 112, UL 746A |
|
Nilit Nilamid A3 H6 G5 25% Glass Reinforced PA66
Description: Nilamid A3 H6 G5 is a 25% glass fiber reinforced NYLON 66 with a special stabilization system against hot oil and grease. As a result of this stabilization, the material has a brown nat..
|
|||
| Comparative Tracking Index |
500
V <br>@Thickness 3.20 mm
|
500
V <br>@Thickness 0.126 in
|
Sol. A; IEC 112, UL 746A |
|
Nilit Nilamid A3 H6 G6 30% Glass Reinforced PA66
Description: Nilamid A3 H6 G6 is a 30% glass fiber reinforced NYLON 66 with a special stabilization system against hot oil and grease. As a result of this stabilization, the material has a brown nat..
|
|||
| Comparative Tracking Index |
500
V <br>@Thickness 3.20 mm
|
500
V <br>@Thickness 0.126 in
|
Sol. A; IEC 112, UL 746A |
|
Nilit Nilamid B3 H G10 50% Glass Fiber Reinforced PA6
Description: Nilamid B3 H G10 is a product that combines outstanding strength and stiffness with good moldability and good impact strength. It is widely used for structural applications.Key characte..
|
|||
| Comparative Tracking Index |
500
V <br>@Thickness 3.20 mm
|
500
V <br>@Thickness 0.126 in
|
Sol. A; IEC 112, UL 746A |
|
Nilit Nilamid B3 H G3 15% Glass Fiber Reinforced PA6
Description: Nilamid B3 H G3 is a general purpose, 15% glass fiber reinforced NYLON 6. These products combine good overall mechanical performance and impact strength with ease of processing. Key cha..
|
|||
| Comparative Tracking Index |
500
V <br>@Thickness 3.20 mm
|
500
V <br>@Thickness 0.126 in
|
Sol. A; IEC 112, UL 746A |
|
Nilit Nilamid B3 H G6 30% Glass Fiber Reinforced PA6
Description: Nilamid B3 H G6 is a general purpose, 30% glass fiber reinforced NYLON 6 with a combination of good mechanical performance, impact strength and processability. It is one of the most wid..
|
|||