Electrical Properties Metric English Comments
Comparative Tracking Index >= 600 V
<br>@Thickness 3.20 mm
>= 600 V
<br>@Thickness 0.126 in
Sol. A; IEC 112, UL 746A
Nilit Nilamid A H2 FR HF2 Unfilled, Flame Retardant PA66/6 Co-Polymer
Description: Nilamid A H2 FR HF2 is an unfilled, flame retardant NYLON 66/6 co-polymer that does not contain halogen or red phosphorous. This product combines excellent flow characteristics and extr..
Comparative Tracking Index 600 V
<br>@Thickness 3.20 mm
600 V
<br>@Thickness 0.126 in
Sol. A; IEC 112, UL 746A
Nilit Nilamid A3 H G3 15% Glass Reinforced PA66
Description: Nilamid A3 H G3 is a general purpose, 15% glass fiber reinforced NYLON 66. This product combines good overall mechanical performance and impact strength with ease of processing.Key char..
Comparative Tracking Index 600 V
<br>@Thickness 3.20 mm
600 V
<br>@Thickness 0.126 in
Sol. A; IEC 112, UL 746A
Nilit Nilamid B3N Unfilled, Nucleated PA6
Description: Nilamid B3N is an unfilled, nucleated NYLON 6. It is fast cycling, and combines ease of processing with good overall mechanical characteristics.Key characteristics: Fast cyclingEasy pro..
Comparative Tracking Index 600 V
<br>@Thickness 3.20 mm
600 V
<br>@Thickness 0.126 in
Sol. B; IEC 112, UL 746A
Nilit Nilamid B3N Unfilled, Nucleated PA6
Description: Nilamid B3N is an unfilled, nucleated NYLON 6. It is fast cycling, and combines ease of processing with good overall mechanical characteristics.Key characteristics: Fast cyclingEasy pro..
Comparative Tracking Index 600 V
<br>@Temperature 23.0 °C
600 V
<br>@Temperature 73.4 °F
IEC 60112
DuPont Performance Polymers Crastin® S600F20 BK851 PBT &nbsp;(Unverified Data**)
Crastin® S600F20 BK851 is an unreinforced, lubricated, medium viscosity, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Comparative Tracking Index 600 V
<br>@Temperature 23.0 °C
600 V
<br>@Temperature 73.4 °F
IEC 60112
DuPont Performance Polymers Crastin® S600F40 NC010 PBT &nbsp;(Unverified Data**)
Crastin® S600F40 NC010 is an unreinforced, lubricated, low viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Comparative Tracking Index 600 V
<br>@Temperature 23.0 °C
600 V
<br>@Temperature 73.4 °F
IEC 60112
DuPont Performance Polymers Crastin® S620F20 BK851 PBT &nbsp;(Unverified Data**)
Crastin® S620F20 BK851 is an unreinforced, nucleated, lubricated, medium viscosity, black polybutylene terephthalate resin for fast injection molding.Information provided by DuPont Performance Poly..
Comparative Tracking Index 600 V
<br>@Thickness 3.20 mm
600 V
<br>@Thickness 0.126 in
Sol. A; IEC 112, UL 746A
Nilit Nilamid A3 H ZB High Impact PA66
Description: Nilamid A3 H ZB is high impact NYLON 66. The product maintains excellent impact properties, even at minus temperatures, whilst maintaining mechanical characteristics. Application areas ..
Comparative Tracking Index 600 V
<br>@Thickness 3.20 mm
600 V
<br>@Thickness 0.126 in
Sol. B; IEC 112, UL 746A
Nilit Nilamid A3 H ZC High Impact PA66
Description: Nilamid A3 H ZC has outstanding impact performance, even at minus temperatures. It is widely used for components subjected to high shock loads. Applications include bicycle components, ..
Comparative Tracking Index 600 V
<br>@Thickness 3.20 mm
600 V
<br>@Thickness 0.126 in
Sol. A; IEC 112, UL 746A
Nilit Nilamid A3 H ZE High Impact PA66
Description: Nilamid A3 H ZE was developed for applications which are subjected to very high shock loads, also at minus temperatures. It has good impact performance, whilst maintaining good strength..
Comparative Tracking Index 600 V
<br>@Thickness 3.20 mm
600 V
<br>@Thickness 0.126 in
Sol. B; IEC 112, UL 746A
Nilit Nilamid A3 H ZE High Impact PA66
Description: Nilamid A3 H ZE was developed for applications which are subjected to very high shock loads, also at minus temperatures. It has good impact performance, whilst maintaining good strength..
Comparative Tracking Index 600 V
<br>@Thickness 3.20 mm
600 V
<br>@Thickness 0.126 in
Sol. A; IEC 112, UL 746A
Nilit Nilamid A3 N H2 Nucleated, Heat Stabilized Nylon 66
Description: Nilamid A3 N H2 is a nucleated, heat stabilized NYLON 66 with excellent flow characteristics and very fast cycle time. It is widely used throughout many industries for mass production a..
Comparative Tracking Index 600 V
<br>@Thickness 3.20 mm
600 V
<br>@Thickness 0.126 in
Sol. A; IEC 112, UL 746A
Nilit Nilamid B FR HF Unfilled, Flame Retardant, Halogen and Red Phosphorous Free PA6
Description: Nilamid B FR HF is an unfilled, flame retardant NYLON 6 with excellent flow characteristics, outstanding elongation and impact strength and a good thermal performance. Because of its ex..
Comparative Tracking Index 600 V
<br>@Thickness 3.20 mm
600 V
<br>@Thickness 0.126 in
Sol. A; IEC 112, UL 746A
Nilit Nilamid B3 H XB Unfilled, Impact Resistant PA6
Description: Nilamid B3 H XB is a high impact NYLON 6. The product has excellent impact properties above 0°C, combined with good maintaining mechanical characteristics. Application areas include au..
Comparative Tracking Index 600 V
<br>@Thickness 3.20 mm
600 V
<br>@Thickness 0.126 in
Sol. A; IEC 112, UL 746A
Nilit Nilamid B3 H ZB Unfilled, Low Temperature Impact Resistant PA6
Description: Nilamid B3 H ZB is a high impact NYLON 6. The product has excellent impact properties, even at minus temperatures, whilst maintaining mechanical characteristics. Application areas inclu..
Comparative Tracking Index >= 600 V
<br>@Temperature 23.0 °C
>= 600 V
<br>@Temperature 73.4 °F
DAM; UL 746A
DuPont Performance Polymers Zytel® 103HSL BKB080 Nylon 66 &nbsp;(Unverified Data**)
Zytel® 103HSL BKB080 is a heat stabilized, lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Comparative Tracking Index 600 V
<br>@Temperature 23.0 °C
600 V
<br>@Temperature 73.4 °F
DAM; UL 746A
DuPont Performance Polymers Zytel® 45HSB NC010 Nylon 66 &nbsp;(Unverified Data**)
Zytel® 45HSB NC010 is a high viscosity, heat stabilized polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers
Comparative Tracking Index >= 600 V
<br>@Thickness 3.00 mm,<br> Temperature 23.0 °C
>= 600 V
<br>@Thickness 0.118 in,<br> Temperature 73.4 °F
DAM; UL 746A
DuPont Performance Polymers Zytel® 70G30L NC010 Nylon 66 &nbsp;(Unverified Data**)
Zytel® 70G30L NC010 is a 30% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Comparative Tracking Index 600 V
<br>@Thickness 3.00 mm,<br> Temperature 23.0 °C
600 V
<br>@Thickness 0.118 in,<br> Temperature 73.4 °F
DAM; UL 746A
DuPont Performance Polymers Zytel® 70G30L NC010 Nylon 66 &nbsp;(Unverified Data**)
Zytel® 70G30L NC010 is a 30% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Comparative Tracking Index 600 V
<br>@Temperature 23.0 °C
600 V
<br>@Temperature 73.4 °F
DAM; IEC 60112
DuPont Performance Polymers Zytel® E53 NC010 Nylon 66 &nbsp;(Unverified Data**)
Zytel® E53 NC010 is a very high viscosity polyamide 66 resin for extrusion.Information provided by DuPont Performance Polymers
Comparative Tracking Index 600 V
<br>@Temperature 23.0 °C
600 V
<br>@Temperature 73.4 °F
DAM; IEC 60112
DuPont Performance Polymers Zytel® 151 NC010 Nylon 612 &nbsp;(Unverified Data**)
Zytel® 151 NC010 is a PA 612 resin.Information provided by DuPont Performance Polymers
Comparative Tracking Index >= 600 V
<br>@Temperature 23.0 °C
>= 600 V
<br>@Temperature 73.4 °F
DAM; ASTM D3638
DuPont Performance Polymers Zytel® 151 NC010 Nylon 612 &nbsp;(Unverified Data**)
Zytel® 151 NC010 is a PA 612 resin.Information provided by DuPont Performance Polymers
Comparative Tracking Index 600 V
<br>@Temperature 23.0 °C
600 V
<br>@Temperature 73.4 °F
50%RH; IEC 60112
DuPont Performance Polymers Zytel® 7301 NC010 Nylon 6 &nbsp;(Unverified Data**)
Zytel® 7301 NC010 is a general purpose, unlubricated polyamide 6 resin for extrusion applications.Information provided by DuPont Performance Polymers
Comparative Tracking Index 600 V
<br>@Temperature 23.0 °C
600 V
<br>@Temperature 73.4 °F
DAM; IEC 60112
DuPont Performance Polymers Zytel® 77G33HS1L NC010 Nylon 612
Zytel® 77G33HS1L NC010 is a 33% glass fiber reinforced, heat stabilized polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers
Comparative Tracking Index 600 V
<br>@Temperature 23.0 °C
600 V
<br>@Temperature 73.4 °F
DAM; IEC 60112
DuPont Performance Polymers Zytel® ST801AW BK195 Nylon 66 &nbsp;(Unverified Data**)
Zytel® ST801AW BK195 is a Super Tough, weatherable, easy flow and processing friendly, black polyamide 66 resin for injection molding. It offers the best resistance to outdoor exposure.Information..
Comparative Tracking Index 600 V
<br>@Temperature 23.0 °C
600 V
<br>@Temperature 73.4 °F
DAM; UL 746A
DuPont Performance Polymers Zytel® ST801AW BK195 Nylon 66 &nbsp;(Unverified Data**)
Zytel® ST801AW BK195 is a Super Tough, weatherable, easy flow and processing friendly, black polyamide 66 resin for injection molding. It offers the best resistance to outdoor exposure.Information..
Comparative Tracking Index 600 V
<br>@Temperature 23.0 °C
600 V
<br>@Temperature 73.4 °F
DAM; IEC 60112
DuPont Performance Polymers Zytel® ST801 NC010A Nylon 66 &nbsp;(Unverified Data**)
Zytel® ST801 is an unreinforced, super tough polyamide 66 for injection molding and extrusion. It offers outstanding break resistance over a wide temperature and humidity range and high productivit..
Comparative Tracking Index >= 600 V
<br>@Thickness 3.00 mm,<br> Temperature 23.0 °C
>= 600 V
<br>@Thickness 0.118 in,<br> Temperature 73.4 °F
DAM; UL 746A
DuPont Performance Polymers Zytel® 77G43L NC010 Nylon 612 &nbsp;(Unverified Data**)
Zytel® 77G43L NC010 is a 43% glass fiber reinforced polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers
Comparative Tracking Index 600 V
<br>@Temperature 23.0 °C
600 V
<br>@Temperature 73.4 °F
DAM; IEC 60112
DuPont Performance Polymers Zytel® EFE1068 NC010T Nylon 66 &nbsp;(Unverified Data**)
Zytel® EFE1068 NC010T is a lubricated polyamide 66 for injection molding. It has excellent flow characteristics and was developed for fast production cycles and high productivity applications.Info..
Comparative Tracking Index >= 600 V
<br>@Temperature 23.0 °C
>= 600 V
<br>@Temperature 73.4 °F
DAM; UL 746A
DuPont Performance Polymers Zytel® EFE1068 NC010T Nylon 66 &nbsp;(Unverified Data**)
Zytel® EFE1068 NC010T is a lubricated polyamide 66 for injection molding. It has excellent flow characteristics and was developed for fast production cycles and high productivity applications.Info..