| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Comparative Tracking Index |
600
V <br>@Thickness 3.20 mm
|
600
V <br>@Thickness 0.126 in
|
Sol. A; IEC 112, UL 746A |
|
Nilit Nilamid A G5 FR PH2 25% Glass Fiber Reinforced, Flame Retardant PA66 (with Red Phosphorous)
Description: Nilamid A G5 FR PH2 combines flame retardancy with outstanding mechanical performance. This product has a complete yellow card, with RTI and CTI listings. The formulation has been optim..
|
|||
| Comparative Tracking Index |
600
V <br>@Thickness 3.20 mm
|
600
V <br>@Thickness 0.126 in
|
Sol. A; IEC 112, UL 746A |
|
Nilit Nilamid A3 H G3 15% Glass Reinforced PA66
Description: Nilamid A3 H G3 is a general purpose, 15% glass fiber reinforced NYLON 66. This product combines good overall mechanical performance and impact strength with ease of processing.Key char..
|
|||
| Comparative Tracking Index |
600
V <br>@Thickness 3.20 mm
|
600
V <br>@Thickness 0.126 in
|
Sol. A; IEC 112, UL 746A |
|
Nilit Nilamid B3N Unfilled, Nucleated PA6
Description: Nilamid B3N is an unfilled, nucleated NYLON 6. It is fast cycling, and combines ease of processing with good overall mechanical characteristics.Key characteristics: Fast cyclingEasy pro..
|
|||
| Comparative Tracking Index |
600
V <br>@Thickness 3.20 mm
|
600
V <br>@Thickness 0.126 in
|
Sol. A; IEC 112, UL 746A |
|
Nilit Nilitop BT N Unfilled, Nucleated PBT
Description: Nilitop BT N is an unfilled, nucleated PBT that has excellent cycle times.Key characteristics: Good overall mechanical performanceLow moisture absorptionExcellent UV resistanceExcellent..
|
|||
| Comparative Tracking Index |
600
V <br>@Temperature 23.0 °C
|
600
V <br>@Temperature 73.4 °F
|
IEC 60112 |
|
DuPont Performance Polymers Crastin® S600F20 BK851 PBT
(Unverified Data**)
Crastin® S600F20 BK851 is an unreinforced, lubricated, medium viscosity, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
|
|||
| Comparative Tracking Index |
600
V <br>@Temperature 23.0 °C
|
600
V <br>@Temperature 73.4 °F
|
IEC 60112 |
|
DuPont Performance Polymers Crastin® S600F20 NC010 PBT
(Unverified Data**)
Crastin® S600F20 NC010 is an unreinforced, lubricated, medium viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
|
|||
| Comparative Tracking Index |
600
V <br>@Thickness 3.20 mm
|
600
V <br>@Thickness 0.126 in
|
Sol. A; IEC 112, UL 746A |
|
Nilit Nilamid A3 H ZB High Impact PA66
Description: Nilamid A3 H ZB is high impact NYLON 66. The product maintains excellent impact properties, even at minus temperatures, whilst maintaining mechanical characteristics. Application areas ..
|
|||
| Comparative Tracking Index |
600
V <br>@Thickness 3.20 mm
|
600
V <br>@Thickness 0.126 in
|
Sol. B; IEC 112, UL 746A |
|
Nilit Nilamid A3 H ZB High Impact PA66
Description: Nilamid A3 H ZB is high impact NYLON 66. The product maintains excellent impact properties, even at minus temperatures, whilst maintaining mechanical characteristics. Application areas ..
|
|||
| Comparative Tracking Index |
600
V <br>@Thickness 3.20 mm
|
600
V <br>@Thickness 0.126 in
|
Sol. A; IEC 112, UL 746A |
|
Nilit Nilamid A3 H ZC High Impact PA66
Description: Nilamid A3 H ZC has outstanding impact performance, even at minus temperatures. It is widely used for components subjected to high shock loads. Applications include bicycle components, ..
|
|||
| Comparative Tracking Index |
600
V <br>@Thickness 3.20 mm
|
600
V <br>@Thickness 0.126 in
|
Sol. B; IEC 112, UL 746A |
|
Nilit Nilamid A3 H ZC High Impact PA66
Description: Nilamid A3 H ZC has outstanding impact performance, even at minus temperatures. It is widely used for components subjected to high shock loads. Applications include bicycle components, ..
|
|||
| Comparative Tracking Index |
600
V <br>@Thickness 3.20 mm
|
600
V <br>@Thickness 0.126 in
|
Sol. A; IEC 112, UL 746A |
|
Nilit Nilamid A3 H ZE High Impact PA66
Description: Nilamid A3 H ZE was developed for applications which are subjected to very high shock loads, also at minus temperatures. It has good impact performance, whilst maintaining good strength..
|
|||
| Comparative Tracking Index |
600
V <br>@Thickness 3.20 mm
|
600
V <br>@Thickness 0.126 in
|
Sol. B; IEC 112, UL 746A |
|
Nilit Nilamid A3 H ZE High Impact PA66
Description: Nilamid A3 H ZE was developed for applications which are subjected to very high shock loads, also at minus temperatures. It has good impact performance, whilst maintaining good strength..
|
|||
| Comparative Tracking Index |
600
V <br>@Thickness 3.20 mm
|
600
V <br>@Thickness 0.126 in
|
Sol. A; IEC 112, UL 746A |
|
Nilit Nilamid A3 N H2 Nucleated, Heat Stabilized Nylon 66
Description: Nilamid A3 N H2 is a nucleated, heat stabilized NYLON 66 with excellent flow characteristics and very fast cycle time. It is widely used throughout many industries for mass production a..
|
|||
| Comparative Tracking Index |
600
V <br>@Thickness 3.20 mm
|
600
V <br>@Thickness 0.126 in
|
Sol. A; IEC 112, UL 746A |
|
Nilit Nilamid B FR HF Unfilled, Flame Retardant, Halogen and Red Phosphorous Free PA6
Description: Nilamid B FR HF is an unfilled, flame retardant NYLON 6 with excellent flow characteristics, outstanding elongation and impact strength and a good thermal performance. Because of its ex..
|
|||
| Comparative Tracking Index |
600
V <br>@Thickness 3.20 mm
|
600
V <br>@Thickness 0.126 in
|
Sol. A; IEC 112, UL 746A |
|
Nilit Nilamid B3 H XB Unfilled, Impact Resistant PA6
Description: Nilamid B3 H XB is a high impact NYLON 6. The product has excellent impact properties above 0°C, combined with good maintaining mechanical characteristics. Application areas include au..
|
|||
| Comparative Tracking Index |
600
V <br>@Thickness 3.20 mm
|
600
V <br>@Thickness 0.126 in
|
Sol. A; IEC 112, UL 746A |
|
Nilit Nilamid B3 H ZB Unfilled, Low Temperature Impact Resistant PA6
Description: Nilamid B3 H ZB is a high impact NYLON 6. The product has excellent impact properties, even at minus temperatures, whilst maintaining mechanical characteristics. Application areas inclu..
|
|||
| Comparative Tracking Index |
600
V <br>@Temperature 23.0 °C
|
600
V <br>@Temperature 73.4 °F
|
DAM; UL 746A |
|
DuPont Performance Polymers Zytel® 103HSL BKB080 Nylon 66
(Unverified Data**)
Zytel® 103HSL BKB080 is a heat stabilized, lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
|
|||
| Comparative Tracking Index |
>=
600
V <br>@Temperature 23.0 °C
|
>=
600
V <br>@Temperature 73.4 °F
|
DAM; UL 746A |
|
DuPont Performance Polymers Zytel® 103HSL BKB080 Nylon 66
(Unverified Data**)
Zytel® 103HSL BKB080 is a heat stabilized, lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
|
|||
| Comparative Tracking Index |
>=
600
V <br>@Temperature 23.0 °C
|
>=
600
V <br>@Temperature 73.4 °F
|
DAM; UL 746A |
|
DuPont Performance Polymers Zytel® 45HSB NC010 Nylon 66
(Unverified Data**)
Zytel® 45HSB NC010 is a high viscosity, heat stabilized polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers
|
|||
| Comparative Tracking Index |
>=
600
V <br>@Thickness 3.00 mm,<br> Temperature 23.0 °C
|
>=
600
V <br>@Thickness 0.118 in,<br> Temperature 73.4 °F
|
DAM; UL 746A |
|
DuPont Performance Polymers Zytel® 70G30L NC010 Nylon 66
(Unverified Data**)
Zytel® 70G30L NC010 is a 30% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
|
|||
| Comparative Tracking Index |
600
V <br>@Temperature 23.0 °C
|
600
V <br>@Temperature 73.4 °F
|
DAM; IEC 60112 |
|
DuPont Performance Polymers Zytel® E53 NC010 Nylon 66
(Unverified Data**)
Zytel® E53 NC010 is a very high viscosity polyamide 66 resin for extrusion.Information provided by DuPont Performance Polymers
|
|||
| Comparative Tracking Index |
600
V <br>@Temperature 23.0 °C
|
600
V <br>@Temperature 73.4 °F
|
DAM; IEC 60112 |
|
DuPont Performance Polymers Zytel® 151 NC010 Nylon 612
(Unverified Data**)
Zytel® 151 NC010 is a PA 612 resin.Information provided by DuPont Performance Polymers
|
|||
| Comparative Tracking Index |
>=
600
V <br>@Temperature 23.0 °C
|
>=
600
V <br>@Temperature 73.4 °F
|
DAM; UL 746A |
|
DuPont Performance Polymers Zytel® 151 NC010 Nylon 612
(Unverified Data**)
Zytel® 151 NC010 is a PA 612 resin.Information provided by DuPont Performance Polymers
|
|||
| Comparative Tracking Index |
600
V <br>@Temperature 23.0 °C
|
600
V <br>@Temperature 73.4 °F
|
DAM; IEC 60112 |
|
DuPont Performance Polymers Zytel® 77G33HS1L NC010 Nylon 612
Zytel® 77G33HS1L NC010 is a 33% glass fiber reinforced, heat stabilized polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers
|
|||
| Comparative Tracking Index |
600
V <br>@Temperature 23.0 °C
|
600
V <br>@Temperature 73.4 °F
|
DAM; UL 746A |
|
DuPont Performance Polymers Zytel® ST801AW BK195 Nylon 66
(Unverified Data**)
Zytel® ST801AW BK195 is a Super Tough, weatherable, easy flow and processing friendly, black polyamide 66 resin for injection molding. It offers the best resistance to outdoor exposure.Information..
|
|||
| Comparative Tracking Index |
600
V <br>@Temperature 23.0 °C
|
600
V <br>@Temperature 73.4 °F
|
DAM; IEC 60112 |
|
DuPont Performance Polymers Zytel® ST801 NC010A Nylon 66
(Unverified Data**)
Zytel® ST801 is an unreinforced, super tough polyamide 66 for injection molding and extrusion. It offers outstanding break resistance over a wide temperature and humidity range and high productivit..
|
|||
| Comparative Tracking Index |
>=
600
V <br>@Temperature 23.0 °C
|
>=
600
V <br>@Temperature 73.4 °F
|
DAM; UL 746A |
|
DuPont Performance Polymers Zytel® ST801 NC010A Nylon 66
(Unverified Data**)
Zytel® ST801 is an unreinforced, super tough polyamide 66 for injection molding and extrusion. It offers outstanding break resistance over a wide temperature and humidity range and high productivit..
|
|||
| Comparative Tracking Index |
>=
600
V <br>@Thickness 3.00 mm,<br> Temperature 23.0 °C
|
>=
600
V <br>@Thickness 0.118 in,<br> Temperature 73.4 °F
|
DAM; UL 746A |
|
DuPont Performance Polymers Zytel® 77G43L NC010 Nylon 612
(Unverified Data**)
Zytel® 77G43L NC010 is a 43% glass fiber reinforced polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers
|
|||
| Comparative Tracking Index |
600
V <br>@Temperature 23.0 °C
|
600
V <br>@Temperature 73.4 °F
|
DAM; IEC 60112 |
|
DuPont Performance Polymers Zytel® EFE1068 NC010T Nylon 66
(Unverified Data**)
Zytel® EFE1068 NC010T is a lubricated polyamide 66 for injection molding. It has excellent flow characteristics and was developed for fast production cycles and high productivity applications.Info..
|
|||
| Comparative Tracking Index |
>=
600
V <br>@Temperature 23.0 °C
|
>=
600
V <br>@Temperature 73.4 °F
|
DAM; UL 746A |
|
DuPont Performance Polymers Zytel® EFE1068 NC010T Nylon 66
(Unverified Data**)
Zytel® EFE1068 NC010T is a lubricated polyamide 66 for injection molding. It has excellent flow characteristics and was developed for fast production cycles and high productivity applications.Info..
|
|||