Physical Properties Metric English Comments
Density 0.725 - 0.775 g/cc

@Temperature 15.0 °C
0.0262 - 0.0280 lb/in³

@Temperature 59.0 °F
Unipetrol Normal 91 Unleaded MOGAS
Unleaded mogases represent the hydrocarbon blend usually boiling within 20 to 215°C, obtainted from crude oil through distillation and refining processes. They may contain additives that enhance th..
Density 0.725 - 0.775 g/cc

@Temperature 15.0 °C
0.0262 - 0.0280 lb/in³

@Temperature 59.0 °F
Unipetrol Super 95 Unleaded MOGAS
Unleaded mogases represent the hydrocarbon blend usually boiling within 20 to 215°C, obtainted from crude oil through distillation and refining processes. They may contain additives that enhance th..
Density 0.725 - 0.775 g/cc

@Temperature 15.0 °C
0.0262 - 0.0280 lb/in³

@Temperature 59.0 °F
Unipetrol Super plus 98 Unleaded MOGAS
Unleaded mogases represent the hydrocarbon blend usually boiling within 20 to 215°C, obtainted from crude oil through distillation and refining processes. They may contain additives that enhance th..
Density 0.725 g/cc

@Temperature 20.0 °C
0.0262 lb/in³

@Temperature 68.0 °F
ASTM D4052
ExxonMobil IPE Isopropyl Ether
Appearance: Clear/Transparent LiquidAvailability: Asia Pacific and North AmericaInformation provided by ExxonMobil