Physical Properties | Metric | English | Comments |
---|---|---|---|
Coating Weight | 30.7 g/m² | 19.2 lb/ream | ExxonMobil Method |
ExxonMobil Bicor® 220 AB OPP Film Product Description: Bicor AB is a two-side acrylic coated, sealable OPP film designed for general use in overwrap and horizontal packaging. It can be surface printed, reverse printed, or used unpri.. |