Bulk Density 1.43 - 1.59 g/cc
0.0517 - 0.0574 lb/in³
3M #11 Filtration Granule (Corona)
3M #11 Filtration Granules are natural minerals used for water filtration in irrigation system.Information provided by 3M
Bulk Density 1.49 - 1.59 g/cc
0.0538 - 0.0574 lb/in³
3M #11 Roofing Granule (Corona)
3M #11 Grade Roofing Granules are ceramic-coated minerals used as surfacing material in asphalt roofing products. These granules are colored with durable pigments, bonded in a ceramic matrix and tre..
Bulk Density 1.49 - 1.59 g/cc
0.0538 - 0.0574 lb/in³
3M Cool Roofing Granule (Corona)
3M Cool Roofing Granules are ceramic-coated minerals used as surfacing material in asphalt roofing products and are designed specifically to have a higher total solar reflectance than standard granu..
Bulk Density 1.43 - 1.59 g/cc
0.0517 - 0.0574 lb/in³
3M Headlap Roofing Granule (Corona)
3M Headlap Roofing Granules are ceramic-coated or natural minerals used as headlap surfacing material in asphalt roofing products. These granules are treated to promote adhesion to asphalt. These He..