Physical Properties Metric English Comments
Vapor Pressure 0.140 bar

@Temperature 25.0 °C
105 torr

@Temperature 77.0 °F
Solvay Specialty Polymers Galden® HT80 PFPE Heat Transfer Fluid
Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service..