Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 745000 cP @Temperature -26.0 °C |
745000 cP @Temperature -14.8 °F |
ASTM D2983 |
ExxonMobil SpectraSyn™ 100 Polyalphaolefin (PAO) Fluid Product Description: SpectraSyn™ High Viscosity Polyalphaolefin (PAO) basestocks feature low temperature properties (pour point and viscosity), low volatility, and improved thermal stability. Spect.. |