Polymer Property : Izod Impact, Notched = 3.09 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 3.09 J/cm

@Temperature 23.0 °C
5.79 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Noryl PC180X PPE+PS
Nonbrominated, nonchlorinated flame retardant. V-1/5VA rated; 175F (90C) HDT. Improved productivity and reliability.This data was supplied by SABIC-IP for the Americas region.