Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.430 - 4.90 J/cm | 0.806 - 9.19 ft-lb/in | Average value: 2.11 J/cm Grade Count:36 |
Overview of materials for Polypropylene, Mineral Reinforced, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced, Impact Modified". Each property range of values reported is minimum a.. |