Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact Notched | 38.0 - 40.7 J | 28.0 - 30.0 ft-lb | V-Notch |
Latrobe Lescalloy® UT-18 VAC-ARC ; 3.25 in. round High Strength Alloy Steel UT-18 VAC-ARC is a medium-carbon, low-alloy heat resistant steel having high strength to 1000°F. It is used primarily for turbine and compressor rotor shafts. Vacuum consumable electrode melting.. |
|||
Izod Impact Notched | 38.0 - 39.3 J | 28.0 - 29.0 ft-lb | V-Notch |
Latrobe Lescalloy® UT-18 VAC-ARC ; 3.75 in. round High Strength Alloy Steel UT-18 VAC-ARC is a medium-carbon, low-alloy heat resistant steel having high strength to 1000°F. It is used primarily for turbine and compressor rotor shafts. Vacuum consumable electrode melting.. |