Polymer Property : Tensile Strength at Break = 3150 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 21.7 MPa
3150 psi
510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible 1351 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength at Break 21.7 MPa
3150 psi
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible 90067 Polyvinyl Chloride, Flexible (PVC, Flexible)
Automotive OEM approval(s).Information provided by PolyOne
Tensile Strength at Break 21.7 MPa
3150 psi
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible XV3860 Polyvinyl Chloride, Flexible (PVC, Flexible)
All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high ..
Tensile Strength at Break 21.7 MPa
3150 psi
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible R267AM Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength at Break 21.7 MPa
3150 psi
ASTM D638
Teknor Apex APEX® 3601-85 Polyvinyl Chloride, Flexible
Uses: Medical/Healthcare Applications Agency Ratings: NSF 61 Forms: Pellets Additional Information: Second Generation SeriesInformation Provided by Teknor Apex
Tensile Strength at Break 21.7 MPa
3150 psi
ASTM D638
Teknor Apex APEX® 01-A0303E-95 Polyvinyl Chloride, Flexible
Notes: 105°C Insulation; RoHS Compliant Uses: Automotive Electronics; Insulation; Wire and Cable Applications Wire Types: GPT Agency Ratings: SAE J1128 Forms: PelletsInformation Provided by Tekno..
Tensile Strength at Break 21.7 MPa
3150 psi
ASTM D638
Plastics Group Polifil® RMC-40V 40% Calcium Carbonate-Reinforced Polypropylene, High Impact, UV Stabilized
Polifil® RMC-V series compounds are high impact, UV stabilized polypropylenes reinforced with fine particle size calcium carbonate. In addition to the highest impact possible, these compounds retar..
Tensile Strength at Break 21.7 MPa
3150 psi
ASTM D3759
3M 3380 HVAC Construction
General purpose aluminum foil tape. Go to product for this market. UL 723 Classified.Information provided by 3M