Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rigidity | 70.4 GPa @Temperature 482 °C |
10200 ksi @Temperature 900 °F |
|
Latrobe BG42® Stainless Knife Steel (AMS 5749) LESCALLOY® BG42® VIM VAR is a double vacuum melted martensitic stainless high speed steel designed for critical aerospace structural components and high performance bearings. The steel is vacu.. |