Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 78.0 MPa @Strain 0.200 %, Temperature 600 °C |
11300 psi @Strain 0.200 %, Temperature 1110 °F |
EN min.; EN 10002-5 |
Outokumpu 4948 High Temperature Austenitic Stainless Steel Creep-resistant variant of 1.4301, with a standardized minimum carbon content for service at temperatures of up to 800°C in dry air.Applications: Heat and creep resistance. For use over 550°C for.. |