Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 313.8 MPa | >= 45510 psi | |
Crucible Steel SIL10 Martensitic Steel Information provided by Crucible Specialty Metals. |
|||
Tensile Strength, Yield | >= 313.8 MPa | >= 45510 psi | |
Crucible Steel TPA21 Martensitic Steel Information provided by Crucible Specialty Metals. |