Polymer Property : Tensile Modulus = 5.65 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 5.65 GPa
819 ksi
Plastcom SLOVALEN PH 59 GF 30 PP, 30% glass fibre
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fibre, with high strength, rigidity and toughness, adapted thermal properties, decreased shrinkage. Suita..
Tensile Modulus 5.65 GPa
819 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP DF004ER PC
LNP THERMOCOMP* DF004ER is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Easy Molding. Mold Release.