Mechanical Properties Metric English Comments
1% Secant Modulus, TD 191 MPa
27700 psi
ASTM D882
Chevron Phillips MarFlex® D139DK Metallocene Linear Low Density Polyethylene, Blown Film
This mLLDPE is tailored for applications that require:Excellent clarityExcellent glossExcellent toughnessExcellent heat sealTypical blown film applications include:Seal layer in coextrusionsHeavy du..
1% Secant Modulus, TD 191 MPa
27700 psi
ASTM D882
Chevron Phillips MarFlex® D139FK Metallocene Linear Low Density Polyethylene, Blown Film
This mLLDPE is tailored for applications that require:Excellent clarityExcellent glossExcellent toughnessExcellent heat sealTypical blown film applications include:Seal layer in coextrusionsHeavy du..