Polymer Property : Tensile Strength, Ultimate = 2.56 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 2.56 MPa
371 psi
ASTM D 638
REXtac Rextac® RT 2180 Amorphous Polyalphaolefin (APAO)
Adhesive and Sealant Grade.Description: Propylene homopolymer and FDA compliantFeatures: High softening point, short open time, good cohesive strength, and high viscosityApplications: Component of h..