Tensile Strength, Ultimate 53.4 MPa
7750 psi
ASTM D638
Plenco 7300 Phenolic, Nodular, Transfer Molded  (discontinued **)
Two-Stage Phenolic. PLENCO 07300 is an organic fiber reinforced phenolic molding compound offering improved mechanical strength and excellent cosmetic properties. UL recognized under component file..
Tensile Strength, Ultimate 53.4 MPa
7750 psi
after optimum cure
Armstrong A-271 Epoxy Adhesive
A clear amber adhesive system. A-271 is a medium viscosity liquid with excellent wetting ability. It is ideal for bonding glass or similar smooth surfaces. It features very low shrinkage coupled ..
Tensile Strength, Ultimate 53.4 MPa
7750 psi
ASTM D638
Ensinger ENSIKEM® PVDF (Polyvinylidene Fluoride) - Extruded Products  (discontinued **)
Polyvinylidene fluoride, or PVDF, is a fluorinated thermoplastic resin that has outstanding resistance to most mineral and organic acids, aliphatic and aromatic hydrocarbons, alcohols, halogenated s..
Tensile Strength, Ultimate 53.4 - 86.0 MPa
7750 - 12500 psi
Average value: 66.8 MPa Grade Count:5
Overview of materials for Polycarbonate, Glass Fiber & Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber & Bead Filled". Each property range of values reported is minimum and maximum..