Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.21 GPa | 900 ksi | ASTM D790 |
Niche Polymer PA66GM40BK Nylon 66, 40% Mineral Fiber Filled Information provided by Niche Polymer |
|||
Flexural Modulus | 6.21 GPa | 900 ksi | ASTM D790 |
Quadrant EPP Ketron® CM GF30 Compression Molded, 30% Glass Reinforces Polyethererther Ketone(ASTM Product Data Sheet) |
|||
Flexural Modulus | 6.21 GPa | 900 ksi | ASTM D790 |
Polymer Resources NY66-M40 Nylon 66, 40% Mineral Filled Nylon 66, 40% Mineral Filled, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested.. |
|||
Flexural Modulus | 6.21 GPa | 900 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1033HL Nylon 6/6 (Cond) Information provided by Ravago. |
|||
Flexural Modulus | 6.21 GPa | 901 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® A-1230 L Polyphthalamide (PPA)
(discontinued **) Amodel A-1230 L is a 30% mineral filled polyphthalamide (PPA) that offers low warpage and excellent dimensional stability. This resin also has a high deflection temperature, flexural modulus and ten.. |
|||
Flexural Modulus | 6.21 GPa | 900 ksi | ASTM D790 |
Polymer Resources PC/ABS-G30 General Purpose PC/ABS Alloy, 30% Glass Filled PC/ABS Alloy, General Purpose, 30% Glass FilledProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provi.. |
|||
Flexural Modulus | 6.21 GPa @Thickness 3.17 mm |
900 ksi @Thickness 0.125 in |
ASTM D790 |
PTS 30GFR-BK PBT- Flame Retardant, 30% Glass Filled PBT Black Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 6.21 GPa | 900 ksi | ASTM D790 |
Techmer ES Plaslube® J-1/20/TF/20 BK PA66 |
|||
Flexural Modulus | 6.21 GPa | 900 ksi | ASTM D790 |
Techmer ES Electrablend® ABS 03011 FR BK MB 15% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 15% Filler by WeightFeatures: Flame Retardant and Electromagnetic Shielding (EMI)Appearance: BlackTPCI# 7965121I.. |
|||
Flexural Modulus | 6.21 GPa | 900 ksi | ASTM D790 |
Techmer ES Electrablend® ABS SS16 FR BK 16% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 16% Filler by WeightFeatures: Electromagnetic Shielding (EMI)Appearance: BlackInformation provided by TP Composi.. |
|||
Flexural Modulus | 6.21 GPa | 900 ksi | ASTM D790 |
Techmer ES HiFill® HDPE LGF50 12 mm 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 6.21 GPa | 900 ksi | ASTM D790 |
Chase Plastics CP Pryme® N320L (Dry) Nylon 6, 20% Glass Fiber Reinforced, Lubricated, Recycled Content Features: LubricatedRecycled contentForm: PelletsInformation provided by Chase Plastics. |
|||
Flexural Modulus | 6.21 GPa | 900 ksi | ASTM D790 |
Ensinger Tecapeek® XP-100 Compression Molded PEEK Compound, Bearing Grade Material with 10% Graphite, 10% PTFE, and 10% Carbon Fiber Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Flexural Modulus | 6.21 GPa | 900 ksi | Crosswise; ASTM D790 |
Bedford Plastics Glass Reinforced FR Polyester Flat Sheet, 1/8" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Flexural Modulus | 6.21 GPa | 900 ksi | Crosswise; ASTM D790 |
Bedford Plastics Glass Reinforced Vinylester Flat Sheet, 1/8" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Flexural Modulus | 6.21 GPa | 900 ksi | ASTM D790 |
PolyOne Edgetek® AT-25GF/000 Acetal-Copolymer, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 6.21 GPa | 900 ksi | ASTM D790 |
PolyOne Edgetek® MLS-XC195C-2 Polysulfone Alloy - ESD Material - Lubricated