Mechanical Properties Metric English Comments
Modulus of Rupture 0.0310 GPa

@Temperature 649 °C,
Time 3.60e+6 sec
4.50 ksi

@Temperature 1200 °F,
Time 1000 hour
Stress Rupture Strength
AK Steel 13-4 SR® Ferritic Stainless Steel
AK Steel 13-4 SR Stainless Steel is a ductile weldable ferritic with 13% Cr and 3.75% Al. The high aluminum content results in a base alloy with high electrical resistivity. It is intended for use w..