Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | >= 0.0400 kN/m | >= 0.228 pli | |
P & P Technology Polyester Polyurethane Foam Description- High performance acoustic and dust filtration foam with a density of 60 Kg/cubic meter with excellent fire resistance properties. Used in heating, ventilation, electronic, aeronautic, a.. |
|||
Tear Strength | 0.0400 - 10.5 kN/m | 0.228 - 60.0 pli | Average value: 1.08 kN/m Grade Count:71 |
Overview of materials for Thermoset Polyurethane Foam, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Unreinforced". Each property range of values reported is minimum and maximu.. |