Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 140 °C | 284 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® CE1821 PC+ABS High stiffness PC/ABS blend offering high impact, high heat, low CTE, good surface quality and excellent extrusion and thermoforming characteristics. |
|||
Vicat Softening Point | 140 °C | 284 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® 121 PC (Europe-Africa-Middle East) LEXAN 121 is a low viscosity multi purpose grade available in transparent, translucent and opaque colours. |
|||
Vicat Softening Point | 140 °C | 284 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® 923X PC (Asia Pacific) Lexan*923x is a UV stabilized high flow impact modified injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, non-chlorine FR systems, low temperatur.. |
|||
Vicat Softening Point | 140 °C | 284 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® 943X PC Copolymer Lexan* 943X is a UV stabilized medium flow impact modified injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, non-chlorine FR systems, low tempera.. |
|||
Vicat Softening Point | 140 °C | 284 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® CFR9111 PC COPOLYMER (Europe-Africa-Middle East) Lexan* CFR9111 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm and good flow capability. .. |
|||
Vicat Softening Point | 140 °C | 284 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® DMX9455A PC Copolymer (Europe-Africa-Middle East) Lexan* DMX9455A is a standard flow, flame retardant, transparent polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Europe-Africa-Middle East r.. |
|||
Vicat Softening Point | 140 °C | 284 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® EXL6414 PC (Europe-Africa-Middle East) PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 140 °C | 284 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® HF1140R PC High flow grade. Heat stabilized. Enhanced level of mold release. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade will no longer be supported with biocompatib.. |
|||
Vicat Softening Point | 140 °C | 284 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® HP1 PC (Europe-Africa-Middle East) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains mold release. |
|||
Vicat Softening Point | 140 °C | 284 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® HP1NREU PC (Europe-Africa-Middle East) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains no mold release. |
|||
Vicat Softening Point | 140 °C | 284 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Lexan® HPS2S PC Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma steriliza.. |
|||
Vicat Softening Point | 140 °C | 284 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® HPS2S PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma steriliza.. |
|||
Vicat Softening Point | 140 °C | 284 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® ML7652 PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. Medium flow, excellent low temperature ductility.This data was supplied by SABIC-IP for the Americas region. |
|||
Vicat Softening Point | 140 °C | 284 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® OQ1022 PC Standard Flow OQ Resin |
|||
Vicat Softening Point | 140 °C | 284 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® OQ1023 PC (Asia Pacific) Lexan OQ1023 resin is an optical high purity PC resin optimized for demanding recordable and rewritable formats (CD-R, DVD-R, DVD-RW). It is also suitable for short cycletime CD and DVD production |
|||
Vicat Softening Point | 140 °C | 284 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® PC2200 PC (Europe-Africa-Middle East) PC2200 resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release. |
|||
Vicat Softening Point | 140 °C | 284 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® 923X PC Lexan*923x is a UV stabilized high flow impact modified injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, non-chlorine FR systems, low temperatur.. |
|||
Vicat Softening Point | 140 °C | 284 °F | ASTM D1525 |
Mapal Plastics Maplon Type S Polypropylene Sheet Properties: Low stress whitening, Suitable for die cutting, Corona treated on both sides for offset and screen printingApplications: Stationery, Packaging, House-hold productsand printed items |
|||
Vicat Softening Point | 140 °C @Load 5.00 kg |
284 °F @Load 11.0 lb |
|
LATI Laril 13 G/30 PPOm, 30% Glass Fiber Reinforced Modified Polyphenylene Oxide (PPOm) based compound. Glass fibers. Low thermal expansion coefficient. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; .. |
|||
Vicat Softening Point | 140 °C | 284 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics PC2200R PC (Europe-Africa-Middle East) PC2200R resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Vicat Softening Point | 140 °C | 284 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics PC2203R PC PC2203R resin is a high flow (MFR = 22 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was suppli.. |
|||
Vicat Softening Point | 140 °C | 284 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL GFN2 PPE+HIPS (Europe-Africa-Middle East) NORYL GFN2 is a standard 20 % glass fibre reinforced material with a HDT/A of 130C according ISO 75. NORYL GFN2 can be used for all applications where a higher modulus is required. NORYL GFN2 is ava.. |
|||
Vicat Softening Point | 140 °C @Load 5.10 kg |
284 °F @Load 11.2 lb |
50°C/h; ISO 306 |
Covestro Makrolon® ET UV540 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• PC/UV absorber concent.. |
|||
Vicat Softening Point | 140 °C | 284 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL FXN119BK PPE+HIPS Noryl* FXN119BK is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119BKBK is available in black only. |
|||
Vicat Softening Point | 140 °C | 284 °F | ASTM-D1525 |
Polyram RamOfin PPC359T4 Polypropylene, 20% Mineral Filled 20% mineral filled, heat stabilized and impact modified for polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Vicat Softening Point | 140 °C | 284 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Lexan® SD9705 PC Copolymer (Europe-Africa-Middle East) High visocisty PC Copolymer, low smoke, flame retardant resinThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 140 °C | 284 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® VX4915 ASA+PBT (Europe-Africa-Middle East) 15% Glass reinforced nucleated PBT/ASA with excellent mechanical properties high dimensional stability, and low density.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |