Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 221 °C | 430 °F | |
Lubriplate FMO 1700 AW USP Mineral Oil-Based Food Machinery Grade Oil For use where a Class H-1 oil is required. Manufactured in nine ISO grades for a variety of applications. Anti-wear fortified. NOTE: FMO-350AW is also available in a red and orange color which helps.. |
|||
Flash Point | 221 °C | 430 °F | |
Lubriplate H0-2 Petroleum-Based Heavy-Duty Hydraulic Oil Formulated for superior performance, this series contains fluid zinc to effectively reduce ring & vane wear. Excellent anti-rust, anti-corrosion, anti-foam and anti-oxidation properties. High anilin.. |
|||
Flash Point | 221 °C | 430 °F | |
Heatbath/Park 420 Quench Oil 420 Quench Oil is ideal for high alloy steel and distortion-prone parts. It is a "medium-hot", accelerated quench oil used between 200° and 300°F for applications where distortion must be mini.. |
|||
Flash Point | 221 °C | 430 °F | |
Silberline Extra Sparkle Silvex® 300-10-C Sparkle Silvex® C grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited .. |
|||
Flash Point | 221 °C | 430 °F | |
Silberline Silvex® 223-20-C Silvex® C grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited for use .. |
|||
Flash Point | 221 °C | 430 °F | |
Silberline Silvex® 420-15-C Silvex® C grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited for use .. |
|||
Flash Point | 221 °C | 430 °F | |
Silberline Silvex® 440-15-C Silvex® C grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited for use .. |
|||
Flash Point | 221 °C | 430 °F | |
Silberline Sparkle Silvex® 755-20-C Sparkle Silvex® C grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited .. |
|||
Flash Point | 221 °C | 430 °F | |
Silberline Sparkle Silvex® 793-20-C Sparkle Silvex® C grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited .. |
|||
Flash Point | 221 °C | 430 °F | |
Silberline Sparkle Silvex® 883-20-C Sparkle Silvex® C grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited .. |
|||
Flash Point | 221 °C | 430 °F | |
Silberline Sparkle Silvex® 963-30-C Sparkle Silvex® C grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited .. |
|||
Flash Point | 221 °C | 430 °F | |
Silberline Sparkle Silvex® Premier 890-20-C Sparkle Silvex® C grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited .. |
|||
Flash Point | 221 °C | 430 °F | |
Silberline Sparkle Silvex® Premier 950-20-C Sparkle Silvex® C grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited .. |
|||
Flash Point | 221 °C | 430 °F | |
Silberline Silvex® 543-20-C Silvex® C grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited for use .. |
|||
Flash Point | 221 °C | 430 °F | |
Teknor Apex TruVis Esters™ DIDA Di-IsoDecyl Adipate |
|||
Flash Point | 221 °C | 430 °F | ASTM D92 |
ExxonMobil Medium Mobil DTE Oil Named Series The Mobil DTE Oil Named Series of lubricants are premium performance circulating lubricants designed for applications including steam and hydro turbine sets and other systems where long lubricant se.. |
|||
Flash Point | 221 °C | 430 °F | open cup |
Dow Corning 704 DIFFUSION PUMP FLUID A clear, tetramethyltetra-phenyltrisiloxane, single-component fluid for high vacuums of 10-7 to 10-8 torr range (untrapped) and 10-11 (trapped).Information provided by Dow Corning |
|||
Flash Point | 221 °C | 430 °F | |
ChevronTexaco Havoline® SAE 80W-90 Gear Oil Havoline Gear Oils are multipurpose lubricants. They are made from paraffinic base stocks and contain a carefully balanced additive package to provide maximum gear protection and long lubricant life.. |
|||
Flash Point | 221 °C | 430 °F | |
ChevronTexaco Multigear® EP SAE 80W-90 Texaco Multigear EP oils deliver value through:Improved durability — Specially formulated to stand up to the demands of severe service applications.Extended gear life — Extreme pressure properties.. |
|||
Flash Point | 221 °C | 430 °F | |
ChevronTexaco Multigear® LS SAE 80W-90 Texaco Multigear LS delivers value through:Reduced inventory costs — One gear lubricant for both conventional and limited slip differentials. Simplified inventory saves money, space, handling time .. |
|||
Flash Point | 221 °C | 430 °F | ASTM D92 |
ChevronTexaco Supreme LS SAE 80W-90 Supreme LS Gear Lubricant FeaturesChevron Supreme LS Gear Lubricant is a high quality multipurpose gear lubricant.It is formulated with friction modifiers so that it can be used for complete replacement or top-off in limited.. |
|||
Flash Point | 221 °C | 430 °F | ASTM D92 |
ChevronTexaco TEGRA® SAE 75W-90 Synthetic Gear Lubricant FeaturesChevron Tegra Synthetic Gear Lubricants are superior quality, multipurpose gear lubricants.It is manufactured from synthesized hydrocarbon base fluids which have exceptional thermal and oxid.. |
|||
Flash Point | 221 °C | 430 °F | ASTM D92 |
ChevronTexaco Thread Sealing Compound FeaturesChevron Thread Sealing Compound is a time-tested aluminum complex grease designed especially for casing and tubing connections in high-pressure oil well service, or wherever unusually severe.. |
|||
Flash Point | 221 °C | 430 °F | ASTM D92 |
ExxonMobil 797 Mobil DTE 790 Series Mobil DTE 790 Series lubricants are premium performance turbine oils that are engineered to meet the requirements of the most severe steam turbine designs and operation, with maximum oil charge life.. |
|||
Flash Point | 221 °C | 430 °F | ASTM D92 |
ExxonMobil Medium Mobil DTE Oil Named Series The Mobil DTE Oil Named Series of lubricants are premium performance circulating lubricants designed for applications including steam and hydro turbine sets and other systems where long lubricant se.. |
|||
Flash Point | 221 °C | 430 °F | ASTM D92 |
ExxonMobil Mobil 1 75W-140 Gear Lubricant LS Mobil 1 Synthetic Gear Lubricant LS 75W-140 is a supreme performance, synthetic, multi-purpose, automotive gear lubricant designed to meet the highest level performance requirements of many modern p.. |
|||
Flash Point | 221 °C | 430 °F | |
ConocoPhillips Hydroclear® 15W-40 Power-D E.O. 15W-40 Description: Conoco Hydroclear Power-D Engine Oil, formulated from Conoco's premium hydrocracked base stock, protects diesel and gasoline engines against wear, deposits, varnish, rust and corros.. |
|||
Flash Point | 221 °C | 430 °F | ASTM D92 |
ChevronTexaco RPM® SAE 80W-90 Universal Gear Lubricant FeaturesChevron RPM Universal Gear Lubricants are multipurpose lubricants.They are made from paraffinic base stocks and contain a carefully balanced additive package to provide maximum gear protecti.. |
|||
Flash Point | 221 °C | 430 °F | ASTM D92 |
ExxonMobil Mobil 1 75W-140 Gear Lubricant LS Mobil 1 Synthetic Gear Lubricant LS 75W-140 is a supreme performance, synthetic, multi-purpose, automotive gear lubricant designed to meet the highest level performance requirements of many modern p.. |
|||
Flash Point | 221 °C | 430 °F | ASTM D92 |
ExxonMobil 797 Mobil DTE 790 Series Mobil DTE 790 Series lubricants are premium performance turbine oils that are engineered to meet the requirements of the most severe steam turbine designs and operation, with maximum oil charge life.. |