Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.173 - 0.200 W/m-K | 1.20 - 1.39 BTU-in/hr-ft²-°F | Average value: 0.187 W/m-K Grade Count:4 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep.. |
|||
Thermal Conductivity | 0.173 - 0.200 W/m-K | 1.20 - 1.39 BTU-in/hr-ft²-°F | Average value: 0.191 W/m-K Grade Count:5 |
Overview of materials for Polycarbonate, Optical Grade This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | ASTM D177 |
Haysite Heatmeiser® H340 Platen Insulation Haysite’s family of mold and platen insulation products are specially engineered fiberglass reinforced thermoset polyester composites which offer superior energy efficiency, temperature control.. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | ASTM D-2863 |
Saint-Gobain Norton® PMP Film Features/Benefits:Good release properties for up to 180°C (356°F) cure composites (application dependent)low density for high surface area per poundExcellent clarityThermoformableProduct avail.. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® 1804 Polycarbonate MVR (300 °C/1.2 kg) 6.0 cm3/10 minhigh viscosityUV stabilizedoptimized for low plate-outimproved flammabilityUL 94 V-2/1.5 mm and 3.0 mmavailable in transparenttranslucent and opaque colorssolid sh.. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® 1837* Polycarbonate, Impact Grade ISO 7391-PC,MP,(,,)-09-9Global gradeFormerly Makrolon DP1-1837MVR (300 °C/1.2 kg) 11 cm3/10 minImpact modifiedMedium viscosityEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable.. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® 2467 Polycarbonate ISO 7391-PC,MFLR,(,,)-18-9Global gradeFormerly Makrolon DP1-1870MVR (300 °C/1.2 kg) 19 cm3/10 minChlorine- and bromine-free flame retardantUL 94V-2/1.5 mm and 3.0 mmLow viscosityUV stabilizedEasy r.. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® 2656 Polycarbonate ISO 7391-PC,MR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12.5 cm3/10 minFood contact qualityMedium viscosityEasy releaseGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CAv.. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® 2665 Polycarbonate, Flame Retardant Grade ISO 7391-PC,MFR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12.5 cm3/10 minChlorine- and bromine-free flame retardantUL 94V-2/1.5 mm and 3.0 mmMedium viscosityEasy releaseInjection molding - Melt temp.. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® 2667 Polycarbonate, Flame Retardant Grade ISO 7391-PC,MFLR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12.5 cm3/10 minChlorine- and bromine-free flame retardantUL 94V-2/1.5 mm and 3.0 mmMedium viscosityUV stabilizedEasy releaseInjection moldi.. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® 2806 Polycarbonate ISO 7391-PC,M,(,,)-09-9MVR (300 °C/1.2 kg) 9.5 cm3/10 minFood contact qualityMedium viscosityGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CAvailable in transparenttran.. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® 2856 Polycarbonate ISO 7391-PC,MR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 9.5 cm3/10 minFood contact qualityMedium viscosityEasy releaseGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CAva.. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® 2867 Polycarbonate, Flame Retardant Grade ISO 7391-PC,MFLR,(,,)-09-9MVR (300 °C/1.2 kg) 9.5 cm3/10 minChlorine- and bromine-free flame retardantUL 94V-2/1.5 mm and 3.0 mmMedium viscosityUV stabilizedEasy releaseInjection molding - Melt tem.. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® 3106 Polycarbonate ISO 7391-PC,M,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minFood contact qualityHigh viscosityGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CExtrusionAvailable.. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® 3156 Polycarbonate ISO 7391-PC,MR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minFood contact qualityHigh viscosityEasy releaseGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CExtru.. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® 6265 Polycarbonate, Flame Retardant Grade ISO 7391-PC,MFR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 19 cm3/10 minFlame retardantUL 94V-0/1.5 mmLow viscosityEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in opaque co.. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® 6455 Polycarbonate, Flame Retardant Grade MVR (300 °C/1.2 kg) 12.5 cm3/10 minUL 94V-0/3.0 mmeasy releaseinjection moldingavailable in transparenttranslucent and opaque colorsPreprocessingMax. Water content |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® AL2447 Polycarbonate ISO 7391-PC,MLR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 19 cm3/10 minAutomotive lightingLow viscosityUV stabilizedEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in transpa.. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® LED2045 Polycarbonate ISO 7391-PC,MRT,(,,)-24-9Global gradeMVR (250 °C/2.16 kg) 16.5 cm3/10minLight guidesPC with highest transmissionLow viscosityEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable .. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® LTG3123 Polycarbonate PreprocessingMax. Water content |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® T7855 Polycarbonate, Impact Grade ISO 7391-PC,MPR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12 cm3/10 minImpact modifiedMedium viscosityEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in opaque colors onlyPre.. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® WB1239 Polycarbonate ISO 7391-PC,B,(,,)-05-9Global gradeMVR (300 °C/1.2 kg) 2.5 cm3/10 minBlow moldingHigh viscosityBranchedFood contact qualityExtrusion blow moldingInjection stretch blow moldingAvailable in transpare.. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® 1243 Polycarbonate ISO 7391-PC,ELS,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minExtrusionHigh viscosityBranchedUV stabilizedEasy releaseAvailable in color code 550111onlyMulti wall sheet/profilesPreprocessi.. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® 6487 Polycarbonate, Flame Retardant Grade ISO 7391-PC,MFLR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12.5 cm3/10 minFlame retardantUL 94V-0/1.5 mm and 5VA/3.0 mmMedium viscosityUV stabilizedEasy releaseInjection molding - Melt temperature 2.. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® DP1-1825* Polycarbonate, Impact Grade Developmental productISO 7391-PC,MP,(,,)-09-9MVR (300 °C/1.2 kg) 6.0 cm3/10 minImpact modifiedHigh viscosityInjection molding - Melt temperature 280 - 320 °CAvailable in opaque colors onlyPreproce.. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® DP1-1843* Polycarbonate ISO 7391-PC,RL,(,,)-09-9Developmental productMVR (300 °C/1.2 kg) 9.5 cm3/10 minMedium viscosityUV stabilizedRotomoldingAvailable in transparent and translucent colorsGlobe lightsAs of 1 September 2.. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® OD2015 Polycarbonate Global gradeOptical storage mediaLow viscosityEasy releaseHigh purityInjection moldingAvailable in natural color onlyPreprocessingMax. Water content |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® Rx2530 Polycarbonate ISO 7391-PC,M,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 14.5 cm3/10 minMedical devicessuitable for sterilization with high-energy radiationComplies with the requirements of FDA-modified ISO 10993-1 .. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® Rx1452 Polycarbonate ISO 7391-PC,M,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minMedical devicesLipid resistantsuitable for sterilization with high-energy radiationComplies with the requirements of FDA-modifie.. |
|||
Thermal Conductivity | 0.173 - 0.280 W/m-K | 1.20 - 1.94 BTU-in/hr-ft²-°F | Average value: 0.231 W/m-K Grade Count:4 |
Overview of materials for Polyphenylene Ether, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 30% Glass Filled". Specific grades with glass content between 25% and 34% are inclu.. |