Thermal Properties Metric English Comments
Thermal Conductivity 43.2 W/m-K

@Temperature 15.6 °C
300 BTU-in/hr-ft²-°F

@Temperature 60.0 °F
Performance Alloys MoldStar® 21 (PAS 21) Bronze Mold Alloy
Description: MoldStar® 21 bronze alloy provides good bearing qualities and resistance to wear, abrasion, fatigue, deformation and corrosion.Applications: Lifter BladesSlidesGibsWear PlatesEjector S..
Thermal Conductivity 43.2 W/m-K

@Temperature 15.6 °C
300 BTU-in/hr-ft²-°F

@Temperature 60.0 °F
Performance Alloys MoldStar® 22 (PAS 22) Bronze Mold Alloy
Description: MoldStar® 21 bronze alloy provides good bearing qualities and resistance to wear, abrasion, fatigue, deformation and corrosion.Applications: Ejector SleevesLifter BladesThin Wall Appli..