Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 120 °C | 248 °F | Recommended |
Nye Lubricants 176H (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 120 °C | 248 °F | Recommended |
Nye Lubricants 774 (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 120 °C | 248 °F | Recommended |
Nye Lubricants 774MS (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 120 °C | 248 °F | Deflection Temp.; ASTM D648 |
NCMT NanoPAC™ HS404 High Performance Polypropylene Nanocomposite Applications: Electrical AppliancesInformation provided by Nano Composite Materials Technology Limited |
|||
Maximum Service Temperature, Air | 120 °C | 248 °F | |
Precision Polymer Engineering N85U Nitrile Rubber Nitrile Butadiene Rubber (NBR) 75-95 °IRHD. Copolymer of acrylonitrile and butadiene. To meet Aerospace Material Specification DTD458A Grade B1 (specification inactive for new design).Applications.. |
|||
Maximum Service Temperature, Air | 120 °C | 248 °F | Continuous; FRISETTA Test Method |
Nilit FRIANYL A63 GV20 Nylon 6.6 for injection molding, 20% glass fiber reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Maximum Service Temperature, Air | 120 °C | 248 °F | Maximum Operating Temperature |
Piezo Kinetics 552 Lead Zirconate Titanate Piezoelectric Denoted as Navy Type VI, this ceramic is used as sensors that require extremely high dielectric constant and large displacements. PKI 556 material has been slightly modified to give a higher g33 val.. |
|||
Maximum Service Temperature, Air | 120 °C | 248 °F | Continuous; FRISETTA Test Method |
Nilit FRIANYL B63 H Nylon 6 for injection molding Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Maximum Service Temperature, Air | 120 °C | 248 °F | Continuous; FRISETTA Test Method |
Nilit FRIANYL B63 H-SG30 Nylon 6 for injection molding, 30% mineral filled Nylon 6 for injection molding, heat stabilized (dark natural color).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Maximum Service Temperature, Air | 120 °C | 248 °F | |
Lehmann & Voss LUVOCOM® 1-7882 Polyamide 66, with carbon fiber and PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Electrically conductive, suita.. |
|||
Maximum Service Temperature, Air | 120 °C | 248 °F | short term |
Lehmann & Voss LUVOCOM® 80-7580/BK Polyacetal-copolymer, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Maximum Service Temperature, Air | 120 °C | 248 °F | short term |
Lehmann & Voss LUVOCOM® 80-7653 Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Antistatic.No change of electric potential at bearings in case of separation of charge caused b.. |
|||
Maximum Service Temperature, Air | 120 °C | 248 °F | |
Lehmann & Voss LUVOCOM® 1/CF/30/TF/13/SI/2/BK Polyamide 66, with carbon fiber, PTFE, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh.. |
|||
Maximum Service Temperature, Air | 120 °C | 248 °F | |
Lehmann & Voss LUVOCOM® 1-7943 Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Maximum Service Temperature, Air | 120 °C | 248 °F | Continuous |
Schwartz Technical Plastics LAMIGAMID® 200 Polyamide 66, Conditioned Application: bearing bushes, machine parts, gears, linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Maximum Service Temperature, Air | 120 °C | 248 °F | Continuous |
Schwartz Technical Plastics LAMIGAMID® 200 Polyamide 66, Dry Application: bearing bushes, machine parts, gears, linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Maximum Service Temperature, Air | 120 °C | 248 °F | Continuous |
Schwartz Technical Plastics LAMIGAMID® 309 Cast Polyamide 6, Oil Filled, Conditioned Application: slippers, inserts for coupling boxes, wear linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Maximum Service Temperature, Air | 120 °C | 248 °F | Continuous |
Schwartz Technical Plastics MITELA® HD8B Cotton Fabric, Special Quality Application: bearing shells and bearing collarsInformation provided by Schwartz Technical Plastics GmbH |
|||
Maximum Service Temperature, Air | 120 °C | 248 °F | Continuous Use |
Polyram PlusTek PA309G6 Nylon 6.6, 30% Glass Fiber 30% glass fiber reinforced, UV stabilized polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Maximum Service Temperature, Air | 120 °C | 248 °F | Continuous Use |
Polyram PlusTek PA325G5 Nylon 6.6, 25% Glass Fiber, Flame Retardant 25% glass fiber reinforced, flame retardant, halogen free polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Maximum Service Temperature, Air | 120 - 140 °C | 248 - 284 °F | medium time operation |
Zell-Metall Engineering Plastics Zellamid 1115 By special additives, impact strength and abrasion resistance are further improved. We particularly recommend this material for slipper pads for rolling mills.Color: IvoryApplications: slipper pads .. |
|||
Maximum Service Temperature, Air | 120 - 130 °C | 248 - 266 °F | Epoxy Matrix Limit |
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 54%/G1088 Glass/Carbon Fiber Information provided by HexCel |
|||
Maximum Service Temperature, Air | 120 °C | 248 °F | |
Trelleborg E645 EPDM Rubber EPM -- EPDM or Ethylene -- Propylene Rubber. EPM can only be vulcanized by peroxides or radiation; whereas EPDM can be vulcanized conventionally using sulphur.Properties:Excellent inherent high and .. |
|||
Maximum Service Temperature, Air | 120 °C | 248 °F | Continuous use |
Polyram PlusTek RA314G50 Nylon 66 for Injection Molding, 50% Glass Fiber Reinforced, Heat Stabilized 50% Glass fiber reinforced, heat stabilized Nylon 66 for injection molding applications.Information provided by Polyram. |
|||
Maximum Service Temperature, Air | 120 °C | 248 °F | short term; EMS |
EMS-Grivory Grivory® TR 30 LS nat PA* Product description: Grilamid TR 30 LS natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid TR 30 LS natural contains a processing a.. |
|||
Maximum Service Temperature, Air | 120 - 130 °C | 248 - 266 °F | long term; EMS |
EMS-Grivory Grivory® TSGL-60/4 black 9833 PA666-GF60 Product description: Grilon TSGL-60/4 black is based on a heat stabilized semicrystalline Polyamide PA66+PA6 and 60% long glass fibers. Grilon TSGL-60/4 black is characterized by the following key-p.. |
|||
Maximum Service Temperature, Air | 120 °C | 248 °F | |
Epoxyset Epoxibond EB-106 Unfilled Epoxy Adhesive A two-component, unfilled epoxy adhesive used for bonding and small potting applications in the medical, electronics, and aerospace industries.Information provided by Epoxyset Inc. |
|||
Maximum Service Temperature, Air | 120 °C | 248 °F | |
Abatron AboCoat 8401-1 A/B Silver-Filled Electrically Conductive Epoxy Compound AboCoat 8401-1 A/B is a conventional highly-filled coating to produce conductive paths with the highest silver content possible. It requires strict controls. Resistivity may rise to 0.1 ohm/sq under.. |
|||
Maximum Service Temperature, Air | 120 °C | 248 °F | |
Alliance BCN-11 Bonded (Composite) Magnetic Material |
|||
Maximum Service Temperature, Air | 120 °C | 248 °F | |
Chesterton 690 FG Lubricant Description: Chesterton® 690 FG Lubricant is a high-quality, cost-effective penetrating lubricant. Used in food processing, beverage and pharmaceutical plants, 690 FG Lubricant can go where few pro.. |