Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 105 °C | 221 °F | UL Temperature Rating |
PolyOne Geon™ Vinyl Wire & Cable 1802-xx11FRD Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Maximum Service Temperature, Air | 105 °C | 221 °F | UL Temperature Rating |
PolyOne Geon™ Vinyl Wire & Cable W9400L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Maximum Service Temperature, Air | 105 °C | 221 °F | UL Temperature Rating |
PolyOne Geon™ Vinyl Wire & Cable WJCK504L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Maximum Service Temperature, Air | 105 °C | 221 °F | UL Temperature Rating; UL 1581 |
PolyOne OnFlex™ HFFR 310-01 Thermoplastic Elastomer (TPE) OnFlex™ HFFR 310-01 is a non-halogen flame retardant material designed for cable jackets. New Product. Commercial specifications have not been established. - Non-halogen flame retardant - UL62 comp.. |
|||
Maximum Service Temperature, Air | 105 °C | 221 °F | Continuous; FRISETTA Test Method |
Nilit FRIANYL B63 SG40 Nylon 6 for injection molding, 40% mineral filled Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Maximum Service Temperature, Air | 105 °C | 221 °F | Continuous; 5,000 h |
Quadrant EPP Ertalon® 6 PLA PA 6, cast (ISO Data) Unmodified cast nylon 6 grade exhibiting characteristics which come very close to those of Ertalon 66 SA. It combines high strength, stiffness and hardness with good creep and wear resistance, heat .. |
|||
Maximum Service Temperature, Air | 105 °C | 221 °F | |
Karina 900-35/1-AYR-AC-LF Ivory PVC Compound Flame retardant and heavy metal free PVC compound, recommended for insulation of automotive electrical cables for working at the temperature range of -40°C to 105°C.Information provided by Kar.. |
|||
Maximum Service Temperature, Air | 105 °C | 221 °F | |
LATI Laril 13-V1KC PPOm, Mineral Reinforced, Flame Retardant Modified Polyphenylene Oxide (PPOm) based compound. Mineral filler. UL94 V-1 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. High dimensional stability. Good therm.. |
|||
Maximum Service Temperature, Air | 105 °C | 221 °F | |
GEHR Plastics PA 6 C Nylon 6 Cast Very stressed-relieved and high-molecular weight PA6.Temperature resistant from -40° to approx. 100°C and high stiffness, hardness and toughness. The good mechanical characteristics will be ac.. |
|||
Maximum Service Temperature, Air | 105 °C | 221 °F | UL temperature rating; UL 1581 |
SABIC Innovative Plastics NORYL WCA105 PPE-TPE (Europe-Africa-Middle East) Flexible, non-halogenated FR mPPE extrusion grade ideal for evaluation in applications such as wire insulation. Flame retardant performance capable of meeting VW1 and 105C temperature rating requir.. |
|||
Maximum Service Temperature, Air | 105 °C | 221 °F | UL temperature rating; UL 1581 |
SABIC Innovative Plastics NORYL WCA871 PPE-TPE (Asia Pacific) Halogen-free flame retardant Flexible Noryl extrusion grade intended for evaluation in applications such as insulation and cable jacket. Flame retardant performance and mechanical properties capable.. |
|||
Maximum Service Temperature, Air | 105 °C | 221 °F | UL temperature rating; UL 1581 |
SABIC Innovative Plastics NORYL WCA871A PPE Flame retardant performance and mechanical properties capable of meeting UL VW-1 requirement and 105C temperature rating as defined UL1581. UL1581 tests conducted on 1.0mmD wire with AWG28 conductor.. |
|||
Maximum Service Temperature, Air | 105 °C | 221 °F | UL temperature rating; UL 1581 |
SABIC Innovative Plastics NORYL WCA901 PPE-TPE Non-Halogenated flame retardant, flexible Noryl resin intended for evaluation in wire and cable applications, capable of meeting VW-1 and 105°C end use temperature requirements as defined by UL.. |
|||
Maximum Service Temperature, Air | 105 °C | 221 °F | Continuous Use; ASTM D794 |
Teknor Apex APEX® 4111 Polyvinyl Chloride, Flexible Notes: 105°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain Reliefs; Wire and Cable ApplicationsForms: Pellets Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molded Comp.. |
|||
Maximum Service Temperature, Air | 105 °C | 221 °F | Continuous Use; ASTM D794 |
Teknor Apex APEX® 80-C118-R Polyvinyl Chloride, Flexible Notes: 105°C Insulation; RoHS Compliant Uses: Wire and Cable Applications Forms: PelletsInformation Provided by Teknor Apex |
|||
Maximum Service Temperature, Air | 105 °C | 221 °F | Continuous; ASTM D794 |
Teknor Apex APEX® 91-G1386A-73NT Polyvinyl Chloride, Flexible Notes: RoHS Compliant Uses: Medical/Healthcare Applications Forms: PelletsInformation Provided by Teknor Apex |
|||
Maximum Service Temperature, Air | 105 °C | 221 °F | Deflection temperature in bending , load unknown |
Sibur Discar-L PC/ABS Compositional Polymer Composition material PC/ABS with high shock resistance, thermal, light, and atmospheric resistance for structural parts of technical purpose and parts for internal finishing of automobiles. |
|||
Maximum Service Temperature, Air | 105 °C | 221 °F | Deflection temperature in bending , load unknown |
Sibur Discar-SL PC/ABS Compositional Polymer Composition material PC/ABS with low viscosity of melting with high shock resistance, thermal and atmospheric resistance for large, thin wall structural parts of automobile interiors. |
|||
Maximum Service Temperature, Air | 105 °C | 221 °F | ASTM D794 |
Teknor Apex APEX® 02-A0111A-90NT Polyvinyl Chloride, Flexible Notes: RoHS Compliant Forms: PelletsInformation Provided by Teknor Apex |
|||
Maximum Service Temperature, Air | 105 °C | 221 °F | Continuous Use; ASTM D794 |
Teknor Apex APEX® 80853-B Polyvinyl Chloride, Flexible Notes: 105°C Insulation; RoHS Compliant Features: Flame Retardant; Oil Resistant Uses: Insulation; Wire and Cable Applications Agency Ratings: UL 1063; UL 1581; UL 62; UL 83 Forms: Pellets Wire T.. |
|||
Maximum Service Temperature, Air | <= 105 °C | <= 221 °F | |
Sylvin Technologies 6034-85 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Maximum Service Temperature, Air | <= 105 °C | <= 221 °F | |
Sylvin Technologies 6137-85 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Maximum Service Temperature, Air | 105 °C | 221 °F | Continuous Use |
Teknor Apex Telcar® TL-8421 Thermoplastic Elastomer Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Jacketing; Terminal Cable Jacketing; Undergrou.. |
|||
Maximum Service Temperature, Air | 105 °C | 221 °F | Continuous Use |
Teknor Apex Telcar® TL-8431 Thermoplastic Elastomer Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Electrical/Electronic Applications; Industrial Cable Jacketing;.. |
|||
Maximum Service Temperature, Air | 105 °C | 221 °F | |
Master Bond MasterSil 156 Two Part, Low Viscosity Silicone Description: Master Bond MasterSil 156 is a two component, lower viscosity silicone system for high performance potting, encapsulation and sealing. MasterSil 156 combines high temperature resistance.. |
|||
Maximum Service Temperature, Air | 105 °C | 221 °F | |
Tra-Con Tra-Cast 3010 Flexible Clear Epoxy Casting Compound TRA-CAST 3010 is a clear, low viscosity epoxy casting compound recommended for industrial embedding and casting applications where its combination of superior properties, good clarity, long pot life.. |
|||
Maximum Service Temperature, Air | 105 °C | 221 °F | |
Colorite Polymers CS1533UL Wire and Cable Insulation Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Maximum Service Temperature, Air | 105 °C | 221 °F | |
Colorite Polymers Weatherflex™ CS1525WX (NTL01B) Wire and Cable Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Maximum Service Temperature, Air | 105 °C | 221 °F | Deflection temperature; load unknown. |
Abatron AboCast 50-3/AboCure 50-1 Epoxy Data provided by the manufacturer, Abatron, Inc. Honey viscosity, light amber color. Best combination of high strength and versatility for Abatron "VR" Epoxies. Shelf life is 12+ months.Processin.. |
|||
Maximum Service Temperature, Air | 105 °C | 221 °F | Continuous use |
Von Roll Isola IMI Irrathene® 201 Irradiated Polyethylene Film Data provided by Von Roll Isola USA.Produced by electron bombardment of specially formulated polyethylene film used in a wide variety of electrical applications. Irrathene film is nonmelting and hi.. |