Thermal Properties | Metric | English | Comments |
---|---|---|---|
Solidus | 645 °C | 1190 °F | |
Johnson Matthey Matti-phos 15 Alloy for Fluxless Brazing of Copper This alloy gives ductile joints on copper to copper and is used by electrical assemblies such as motors and contacts.Optimum Joint Gap 0.05 - 0.2 mm.AWS A5.8-92 BCuP-5BS EN 1044 1999 CP102; Does not.. |
|||
Solidus | 645 °C | 1190 °F | |
Johnson Matthey Matti-phos 2 Alloy for Fluxless Brazing of Copper This alloy is less expensive than other Matti-phos alloys. It has good flow and ductility, and has the same uses as Copper-flo.Optimum Joint Gap 0.05 - 0.2 mm.AWS A5.8-92 BCuP-6BS EN 1044 1999 CP10.. |
|||
Solidus | 645 °C | 1190 °F | |
Johnson Matthey Matti-phos 6 Alloy for Fluxless Brazing of Copper This alloy is a low melting point free flowing product. Joints are not as ductile as Matti-Phos 15 or Matti-phos 5.Optimum Joint Gap 0.05 - 0.2 mm.AWS A5.8-92 BCuP-4Federal Specification QQ-B-650 B.. |
|||
Solidus | 646 °C | 1190 °F | |
Johnson Matthey Matti-sil 453 Cadmium Free Brazing Alloy Matti-sil 453S has the additions of Silicon which promotes flow and helps produce neat smooth fillets.Optimum Joint Gap 0.05 - 0.15 mm.AWS A5.8-92 BAg-36Equivalent to Engelhard Silvaloy A-45TEquival.. |
|||
Solidus | 643 °C | 1190 °F | |
Johnson Matthey Matti-sil 453S Cadmium Free Brazing Alloy The 45% Silver alloys, with tin and silicon, are more free flowing than Matti-sil 45 and less costly than Matti-sil 56Sn.Optimum Joint Gap 0.05 - 0.15 mm.Federal Specification QQ-B-564 BAg-8aInforma.. |
|||
Solidus | 643 °C | 1190 °F | Melting Point |
Lucas-Milhaupt SIL-FOS 18 Silver/ Copper/ Phosphorus Alloy Applications: Sil-Fos 18 is a moderate cost brazing filler metal suitable for joining copper, brass and bronze alloys where low brazing temperature and free flowing characteristics are required. I.. |
|||
Solidus | 643 °C | 1190 °F | |
Lucas-Milhaupt Silvabraze 33830 Brazing Alloy Silvabraze is used for brazing of copper and copper alloys, brass and bronze. It can also be used on silver, tungsten, and molybdenum. It is primarily used for the joining of copper-to-copper on vib.. |
|||
Solidus | 643 °C | 1190 °F | |
Lucas-Milhaupt Silvalite Brazing Alloy SILVALITE is used for the brazing of copper and copper alloys, brass and bronze. It can also be used on silver, tungsten and molybdenum. It is primarily used for the joining of copper-to-copper on v.. |
|||
Solidus | 643 °C | 1190 °F | |
Lucas-Milhaupt Silvaloy® 2M Brazing Alloy Silvaloy 2M is used for the brazing of copper and copper alloys, brass and bronze. It can also be used on silver, tungsten and molybdenum. It is primarily used for the joining of copper-to-copper on.. |
|||
Solidus | 643 °C | 1190 °F | |
Lucas-Milhaupt Silvaloy® 18M Brazing Alloy Silvaloy 18M is a ternary alloy of silver, phosphorus, and copper approaching the eutectic composition. It is very fluid at brazing temperature and should be used on well fitted joints. Silvaloy 18M.. |
|||
Solidus | 643 °C | 1190 °F | |
Lucas-Milhaupt Silvaloy® 2 Brazing Alloy Silvaloy 2 is used for the brazing of copper and copper alloys, brass and bronze. It can also be used on silver, tungsten and molybdenum. It is primarily used for the joining of copper-to-copper on .. |
|||
Solidus | 643 °C | 1190 °F | |
Lucas-Milhaupt Silvaloy® 5 Brazing Alloy Silvaloy 5 is used for the brazing of copper and copper alloys, brass and bronze. It can also be used on silver, tungsten and molybdenum. It is primarily used for the joining of copper-to-copper on .. |
|||
Solidus | 643 °C | 1190 °F | |
Lucas-Milhaupt Silvaloy® 6 Brazing Alloy Silvaloy 6 is used for the brazing of copper and copper alloys, brass and bronze. It can also be used on silver, tungsten and molybdenum. It should not be used on ferrous and nickel metals or copper.. |
|||
Solidus | 645 °C | 1190 °F | |
Johnson Matthey Matti-phos 5 Alloy for Fluxless Brazing of Copper This alloy offer a good combination of flow and ductility. Like Matti-phos 6 it is used in air conditioning, refrigeration, medical gas pipework and heat exchanger manufacture.Optimum Joint Gap 0.0.. |
|||
Solidus | 643 °C | 1190 °F | |
Lucas-Milhaupt Silvaloy® 15 Brazing Alloy Silvaloy 15 is used for the brazing of copper and copper alloys, brass, and bronze. It can also be used on silver, tungsten and molybdenum. It is very effective for joining pipe and tubing and is wi.. |
|||
Solidus | 644 °C | 1190 °F | |
Materion AlBeMet® AM 162 Extruded Bar, Annealed Mechanical property values below are in the longitudinal direction; transverse values generally lower. This is a powder metallurgical product produced by gas atomization available as rod, bar, tube.. |
|||
Solidus | 644 °C | 1190 °F | |
Materion AlBeMet® AM 162 Rolled Sheet, Annealed Mechanical properties are typical, longitudinal values at RT. AlBeMet® AM 162 is a powder metallurgical product produced by gas atomization available as rod, bar, tube and sheet. These shapes are.. |