Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 827 - 899 °C | 1520 - 1650 °F | Brazing Range |
Lucas-Milhaupt Cerametil 616 Active Metal Brazing BR 616 strip coated with Ti for joining ceramics without metallization.Information provided by Lucas-Milhaupt, Inc.Alloy compositions are for filler metal strip in wrought Cerametil |
|||
Processing Temperature | 827 - 899 °C | 1520 - 1650 °F | Brazing Range |
Lucas-Milhaupt Lucanex 616 Active Metal Brazing Brazing Paste Blended with Ti for active metal brazing of ceramics.Information provided by Lucas-Milhaupt, Inc.Alloy compositions are for filler metal powder in Lucanex paste |