Processing Properties | Metric | English | Comments |
---|---|---|---|
Casting Temperature | 1260 - 1370 °C | 2300 - 2500 °F | Pouring Range |
IBC Advanced Alloys 41C Beryllium Nickel Casting Alloy Beryllium nickel casting alloys are characterized by their steel-like high strength, toughness, and hardness properties. However, unlike the steel alloys, the beryllium nickel alloy system offers th.. |
|||
Casting Temperature | 1260 - 1370 °C | 2300 - 2500 °F | Pouring Range |
IBC Advanced Alloys 42C Beryllium Nickel Casting Alloy Beryllium nickel casting alloys are characterized by their steel-like high strength, toughness, and hardness properties. However, unlike the steel alloys, the beryllium nickel alloy system offers th.. |
|||
Casting Temperature | 1260 - 1370 °C | 2300 - 2500 °F | Pouring Range |
IBC Advanced Alloys 43C Beryllium Nickel Casting Alloy Beryllium nickel casting alloys are characterized by their steel-like high strength, toughness, and hardness properties. However, unlike the steel alloys, the beryllium nickel alloy system offers th.. |
|||
Casting Temperature | 1260 - 1370 °C | 2300 - 2500 °F | Pouring Range |
IBC Advanced Alloys 44C Beryllium Nickel Casting Alloy Beryllium nickel casting alloys are characterized by their steel-like high strength, toughness, and hardness properties. However, unlike the steel alloys, the beryllium nickel alloy system offers th.. |
|||
Casting Temperature | 1260 - 1370 °C | 2300 - 2500 °F | Pouring Range |
IBC Advanced Alloys 46C Beryllium Nickel Casting Alloy Beryllium nickel casting alloys are characterized by their steel-like high strength, toughness, and hardness properties. However, unlike the steel alloys, the beryllium nickel alloy system offers th.. |
|||
Casting Temperature | 1270 - 1370 °C | 2320 - 2500 °F | |
Wieland 1916 Wilaform Gold Hard palladium white gold alloy with beautiful grey color.Applications: casting, chains, laminar decoration, pipes, tubingDental |