Processing Properties Metric English Comments
Mold Temperature 12.0 - 20.0 °C
53.6 - 68.0 °F
Extrusion Blow Molding
SK Chemicals SKYGREEN® PETG 2008 Specially Formulated PET Copolymer Resin
SKYGREEN PETG is an amorphous copolyester in which a certain amount of ethylene glycol is replaced with 1,4-cyclohexane dimethanol (CHDM), which prevent crystallization, leading to improved processa..