Processing Properties | Metric | English | Comments |
---|---|---|---|
Dry Time | 3 - 12 hour | 3 - 12 hour | |
Ravago Manufacturing Americas Hylex® P1018LLT Polycarbonate Information provided by Ravago. |
|||
Dry Time | 3 hour | 3 hour | |
ExxonMobil Vyram™ 9271-65 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic elastomer which complies with FDA regulations for rubber articles intended for repeated use, as well as rubber articles in contact with non-fatty, non-oily foods as closure.. |
|||
Dry Time | >= 3 hour | >= 3 hour | Always recommended, drying time can be reduced when using vacuum ovens. |
LATI LARPEEK 50 K/30 30% Carbon Fiber Reinforced Polyetheretherketone (PEEK)
(Unverified Data**) Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°.. |
|||
Dry Time | 3 - 5 hour | 3 - 5 hour | |
Samyang Triloy® 410N PC/PET alloy, Flame Retardant
(discontinued **) Characteristics:Impact resistantHeat resistantDimensional stabilityProcessabilityFlame retardantApplications:O/A partRear view mirror housingRice cooker baseAll information provided by Samyang |
|||
Dry Time | >= 3 hour | >= 3 hour | Not necessary for reinforced materials. Drying time can be reduced when using vacuum ovens. |
LATI LAPEX A G/30 30% Glass Fiber Reinforced Polyethersulfone (PES) (UL94 V-0)
(Unverified Data**) Description: Lapex A compounds are polyethersulfone (PES) products. They are high temperature compounds offering an interesting combination of properties. Lapex A provides outstanding thermal resist.. |
|||
Dry Time | 3 - 4 hour | 3 - 4 hour | |
Polymer Resources NY66-G13-[color]H Nylon, 13% Glass Reinforced, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Dry Time | 3 - 4 hour | 3 - 4 hour | 48 hours max. |
PTS Tristar® PC-10R-(6) 6 MFI Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Dry Time | >= 3 hour | >= 3 hour | Drying time can be reduced when using vacuum ovens. |
LATI LATISTAT 43/7-02 Low Density Polyethylene (LDPE) Base Conductive Plastic
(discontinued **) Description: Latistat materials have low specific resistivity. They feature partial electrical conductivity. Selected functional additives give materials with low specific resistivity and reasonable.. |
|||
Dry Time | >= 3 hour | >= 3 hour | Not necessary for reinforced materials. Drying time can be reduced when using vacuum ovens. |
LATI LASULF Polysulfone (PSU)
(Unverified Data**) Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi.. |
|||
Dry Time | 3 - 6 hour | 3 - 6 hour | |
LG Chemical LUCEL ST-550 Ultra High Impact POM, Unreinforced LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Dry Time | 3 - 4 hour | 3 - 4 hour | |
LG Chemical LUMILOY GN1306F Injection Molding FR Heat Resistant mPPO Uses include electric/electronic parts. |
|||
Dry Time | 3 - 4 hour | 3 - 4 hour | |
Star Plastics PC/ABSQX7005 Molding Grade PC/ABS Information provided by Star Plastics, Inc. |
|||
Dry Time | 3 - 5 hour | 3 - 5 hour | |
Samyang Trirex® 3027IR Polycarbonate TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
Dry Time | 3 - 4 hour | 3 - 4 hour | |
Samyang Trirex® PC-3022IR 15 MFI Clear Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Dry Time | 3 - 4 hour | 3 - 4 hour | |
Solvay Technyl® A 216 V40 40% Glass Filled Nylon 66 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Dry Time | 3 hour | 3 hour | |
Teknor Apex Sarlink® 3145D Thermoplastic Elastomer A high hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3145D can be processed by injection blow molding, molding or .. |
|||
Dry Time | 3 hour | 3 hour | |
Teknor Apex Sarlink® 3445D Thermoplastic Elastomer A NSF certified, high hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inje.. |
|||
Dry Time | 3 hour | 3 hour | |
Teknor Apex Sarlink® 3460 Thermoplastic Elastomer A NSF certified, low hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inject.. |
|||
Dry Time | 3 hour | 3 hour | |
ExxonMobil Santoprene® 123-40 Thermoplastic Elastomer A hard, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran.. |
|||
Dry Time | 3 - 5 hour | 3 - 5 hour | |
Asia International Enterprise (Hong Kong) 30G3F Polybutylene terephthalate, 15% Glass Fiber Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Dry Time | 3 hour | 3 hour | |
BASF Ultraform® S2320 003 PRO BK 00120 POM Description: Is a POM, is a standard flowing and rapidly freezing grade suitable for standard functional applications.Information provided by BASF |
|||
Dry Time | 3 hour | 3 hour | |
ExxonMobil Vyram™ 9201-45 Thermoplastic Elastomer
(discontinued **) A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character.. |
|||
Dry Time | 3 - 5 hour | 3 - 5 hour | |
Asia International Enterprise (Hong Kong) 30G6 Polybutylene terephthalate, 30% Glass Fiber Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Dry Time | >= 3 hour | >= 3 hour | |
LATI LATISHIELD 90/13-07A-V1 Modified Polyphenylene Oxide (PPOm) Base E.M.I. Shielding Plastic (UL94 V-1)
(di Description: Latishield E.M.I. shielding materials were developed to solve the problem of shielding electromagnetic interferences with plastic components. The answer is a mixture of two different ty.. |