3M 2187 Polyethylene Protective Tapes

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 2187 Polyethylene Protective Tapes.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Polyethylene Protective Tapes 2187 has a high-tack adhesive system to help provide temporary protection of many metals, plastics and painted metal panels with minimum adhesion build up and clean removal.Information provided by 3M
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 1.70 MPa
247 psi
ASTM D3759
Elongation at Break 450 %
450 %
ASTM D3759
Peel Strength 0.153 kN/m
0.875 pli
Adhesion to Steel; ASTM D3330
Descriptive Properties Value Comments
Adhesive Type Acrylic
Appearance Clear