3M 2497ST High-Temperature Tear Resistant Polyester Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 2497ST High-Temperature Tear Resistant Polyester Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ High-Temperature Tear Resistant Polyester Tape 2497ST is designed for use in masking applications where sliver resistance and clean removal are required.Information provided by 3M
Physical Properties Metric English Comments
Thickness 83.8 microns
3.30 mil
ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 113.75 MPa
16498 psi
ASTM D3756
Elongation at Break 112 %
112 %
ASTM D3756
Peel Strength 0.18626 kN/m
1.0625 pli
to Steel
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 149 °C
300 °F
up to 30 mins
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Adhesive Type Rubber/resin
Appearance Clear