3M 253 Silicone Splicing Tape

Category Polymer , Tape
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 253 Silicone Splicing Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Sealing Splicing Tape 253 is a single-coated paper tape with a modified poly liner implemented as a second liner on the FACE SIDE of the tape. This second liner is added to help ensure roll quality, ease of unwind and protection of the adhesive against contamination until the splice is ready to be made.Information provided by 3M
Physical Properties Metric English Comments
Thickness 127 microns
5.00 mil
Total without polyliner; ASTM D3752
191 microns
7.50 mil
Total; ASTM D3752
Mechanical Properties Metric English Comments
Peel Strength 0.53686 kN/m
3.0625 pli
Adhesion to Steel, 90° Peel, 5 in/min, Initial; ASTM D3330
0.701 kN/m
4.00 pli
Adhesion to Steel, 90° Peel, 5 in/min, 24 hour dwell; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 38.0 °C
100 °F
Application
66.0 °C
151 °F
Minimum Service Temperature, Air 10.0 °C
50.0 °F
Application
Descriptive Properties Value Comments
Adhesive Type Silicone