Material Notes:
3M™ High Performance Temporary Surface Protection Tape 2A826 is a very low adhesion temporary protection tape designed for a variety of surface protection applications.Information provided by 3M
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 31.0 MPa
4500 psi
ASTM D3759
Elongation at Break 600 %
600 %
ASTM D3759
Peel Strength 0.0877 kN/m
0.500 pli
Adhesion to Steel; ASTM D3330
Descriptive Properties Value Comments
Adhesive Type Acrylic-Based
Appearance Clear