3M 2A88 Co-Extruded Multi-Polymer Protect Tapes

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 2A88 Co-Extruded Multi-Polymer Protect Tapes.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Co-Extruded Multi-Polymer Protective Tapes have a high-tack adhesive system to help provide temporary protection for a variety of surface protection applications.Information provided by 3M
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 3.10 MPa
450 psi
ASTM D882
Elongation at Break 600 %
600 %
ASTM D882
Peel Strength 0.1643 kN/m
0.9375 pli
Adhesion to Steel; ASTM D3330
Descriptive Properties Value Comments
Adhesive Type Acrylic
Appearance Clear
Users viewing this material also viewed the following: