3M 361 Glass Cloth Tape

Category Polymer , Tape
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 361 Glass Cloth Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Glass Cloth Tape 361 is coated with a silicone adhesive for many applications requiring high temperature resistance, high adhesion and a very strong, abrasion-resistant backing.Information provided by 3M
Physical Properties Metric English Comments
Thickness 137 microns
5.40 mil
Backing; ASTM D3752
191 microns
7.50 mil
Total; ASTM D3752
Mechanical Properties Metric English Comments
Tensile Strength at Break 167.9 MPa
24350 psi
ASTM D3759
Elongation at Break 10 %
10 %
ASTM D3759
Peel Strength 0.4163 kN/m
2.375 pli
Adhesion to Steel; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -54.0 °C
-65.2 °F
Descriptive Properties Value Comments
Adhesive Type Silicone
Appearance White