Material Notes:
A light box or channel letter contains lighting elements that illuminate the front sign face and transmit some light to the viewer. However much of the illumination is reflected or absorbed by other materials in the light box.Information provided by 3M
Physical Properties Metric English Comments
Thickness 140 - 165 microns
5.50 - 6.50 mil
Film and adhesive
216 - 241 microns
8.50 - 9.50 mil
Adhesive and protective top covering
Mechanical Properties Metric English Comments
Tensile Strength at Break 10.6 - 12.5 MPa
1540 - 1810 psi
Thermal Properties Metric English Comments
Minimum Service Temperature, Air 4.50 °C
40.1 °F