3M 4298UV Adhesion Promoter

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 4298UV Adhesion Promoter.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Adhesion Promoter 4298UV is a liquid primer used to improve the adhesion of 3M™ Acrylic Foam Tapes to low surface energy plastics such as thermoplastic olefins (TPO), thermoplastic urethanes (TPU), and polypropylene. A fluorescent dye has been added so that primer coverage can be verified. Since formulations vary for these materials, each application should be verified through testing. 3M adhesion promoter 4298UV is specifically formulated to be used with 3M acrylic foam tapes for automotive applications.Information provided by 3M
Physical Properties Metric English Comments
Viscosity <= 25 cP
<= 25 cP
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature 4.00 - 38.0 °C
12.0 Month

@Temperature 39.2 - 100 °F
0-95% RH
Descriptive Properties Value Comments
Appearance Straw
Drying time 30-90 sec