3M 4F79 Fire Retardant Polyethylene Carpet Protective Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 4F79 Fire Retardant Polyethylene Carpet Protective Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Fire Retardant Polyethylene Carpet Protective Tape 4F79 has a high-tack adhesive system and to help provide temporary protection of carpet during assembly or maintenance of aircraft.Information provided by 3M
Physical Properties Metric English Comments
Thickness 108 microns
4.25 mil
ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 1.70 MPa
247 psi
ASTM D882
Elongation at Break 600 %
600 %
ASTM D882
Peel Strength 0.1643 kN/m
0.9375 pli
Adhesion to Steel; ASTM D3330
Descriptive Properties Value Comments
Adhesive Type Acrylic
Appearance Opaque