3M 5903 Outdoor Masking Poly Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 5903 Outdoor Masking Poly Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Outdoor Masking Poly Tape 5903 is designed for construction, remodeling and maintenance jobs. It is made with heavy duty polyethylene film and synthetic rubber adhesive. It is UV weather resistant and removes cleanly for up to one month with little or no adhesive residue on most opaque surfaces without deteriorating.Information provided by 3M
Physical Properties Metric English Comments
Thickness 191 microns
7.50 mil
ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 19.4 MPa
2810 psi
ASTM D3756
Elongation at Break 72 %
72 %
ASTM D3756
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 78.0 °C
172 °F
Processing Properties Metric English Comments
Shelf Life 18.0 Month
18.0 Month
Descriptive Properties Value Comments
Adhesive Type Synthetic rubber
Appearance Red