3M 8979N Performance Plus Duct Tape Nuclear Grade

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 8979N Performance Plus Duct Tape Nuclear Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Performance Plus Duct Tape 8979N has a unique product construction for indoor and outdoor applications. This tape is removable with little or no adhesive residue from most opaque surfaces up to six months after application. 3M™ Performance Plus Duct Tape 8979N is also resistant to delamination and deterioration when exposed to UV outdoors for up to one year.Information provided by 3M
Physical Properties Metric English Comments
Thickness 307 microns
12.1 mil
ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 20.3 MPa
2950 psi
ASTM D3756
Elongation at Break 19 %
19 %
ASTM D3756
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 93.0 °C
199 °F
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Adhesive Type Rubber
Appearance Red, Slate Blue