Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Dyneon™ Dynamar™ FX 5927 Polymer Processing Additive

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Fluoropolymer
Manufacturer 3M Dyneon™
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Dyneon™ Dynamar™ FX 5927 Polymer Processing Additive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Dynamar™ Polymer Processing Additive FX 5927 is an improved performance PPA as compared to conventional process aids. This free-flowing fluoropolymer based processing additive is designed for use at very low levels to improve processing of thermoplastics. It utilizes unique technology which makes it particularly effective as a processing additive for linear low density polyethylene blown film. At the very low use levels (typically 100 – 800 ppm) necessary to improve processing, it does not detract from the good physical properties associated with high strength plastics. As a processing additive Dynamar FX 5927 can eliminate melt fracture and reduce die build-up, extruder torque and pressure. Through optimization of the extrusion process, FX 5927 may also allow for an increase in output and improved optical properties such as clarity and gloss. This optimization can yield films with enhanced bidirectional physical properties. FX 5927 can also improve sustainability by improving processability of high strength resins, which allows for down-gauging. FX 5927 can be easily incorporated and dispersed into masterbatch form. FX 5927 exhibits an outstanding balance of properties for dispersibility and effectiveness for melt fracture elimination.Features and Benefits:A high performance PPA for use at very low levels in blown film processesIdeal for use in extrusion of a wide range of polyolefin resinsEasily dispersed in compounding resinsRobust performance in the presence of antiblock agents, pigments and other inorganic additivesFast rate of melt fracture eliminationReduces die build-upBroadens extrusion processing capabilities of polyolefin resinsThis 3M product may be used at levels up to 2000 parts per million (ppm) as a polymer processing additive for all polymers intended for use in contact with all food types described in Table 1 of 21 C.F.R. 176.170(c) under Conditions of Use A through H described in Table 2 of 21 C.F.R. 176.170(c).Information provided by the Dyneon division of 3M.
Physical Properties Metric English Comments
Bulk Density 0.689 g/cc
0.0249 lb/in³
Particle Mesh Size <= 10 Mesh
<= 10 Mesh
Descriptive Properties Value Comments
Active Ingredients 96(%)
Color White to Off-White
Form Granular
Inorganic Additives 4(%)
Typical Use Levels 100 - 800 ppm
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved