3M Dyneon™ FEP 6307 R2RZ Fluorinated Ethylene Propylene Fluorothermoplastic Granules

Category Polymer , Thermoplastic , Fluoropolymer , FEP
Manufacturer 3M Dyneon™
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Dyneon™ FEP 6307 R2RZ Fluorinated Ethylene Propylene Fluorothermoplastic Granules.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Dyneon FEP 6307 R2RZ is a special version of Dyneon FEP 6307 wire jacketing grade FEP with an added nucleating agent for improved foaming in gas injection extrusion processes. As the gas expands and begins to form voids, the added nucleating agent in Dyneon FEP 6307 R2RZ acts as a site for void formation. Dyneon FEP 6307 R2RZ is listed by Underwriters Laboratories as a Plenum Cable Component. It is ideal for gas injection extrusion of foamed FEP coaxial cable core.Information provided by Dyneon, A 3M Company
Physical Properties Metric English Comments
Specific Gravity 2.15 g/cc
2.15 g/cc
ASTM D792
Melt Index of Compound 7.5 g/10 min

@Load 5.00 kg,
Temperature 372 °C
7.5 g/10 min

@Load 11.0 lb,
Temperature 702 °F
ASTM D1238
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ASTM D4591
Oxygen Index >= 95 %
>= 95 %
ASTM D2863
Electrical Properties Metric English Comments
Dielectric Constant <= 2.15

@Frequency 1000 - 1.00e+6 Hz
<= 2.15

@Frequency 1000 - 1.00e+6 Hz
ASTM D150
Dissipation Factor <= 0.00030

@Frequency 1000 Hz
<= 0.00030

@Frequency 1000 Hz
ASTM D150
<= 0.00090

@Frequency 1e+6 Hz
<= 0.00090

@Frequency 1e+6 Hz
ASTM D150